MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8202C PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique crystalline structure results in increased strength, stiffness, heat distortion temperature and performance under load as a homopolymer. It also cycles faster while maintaining properties and resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Water Absorption 1.6 %1.6 %24 hour; ISO Test
 9.3 %9.3 %ISO 62
Moisture Absorption at Equilibrium 2.6 %2.6 %23°C/50% R.H.; ISO 62
Relative Viscosity 2.6 cP2.6 cPISO Test; 96 % SAV
Viscosity Measurement 4848Formic Acid
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM Test
Tensile Strength at Break 90.0 MPa13100 psi0.2 in/min; ASTM Test
 25.0 MPa
@Temperature 120 °C
3630 psi
@Temperature 248 °F
ASTM Test
 25.0 MPa
@Temperature 120 °C
3630 psi
@Temperature 248 °F
ISO Data
 35.0 MPa
@Temperature 80.0 °C
5080 psi
@Temperature 176 °F
ISO Data
 35.0 MPa
@Temperature 80.0 °C
5080 psi
@Temperature 176 °F
ASTM Test
 130 MPa
@Temperature -40.0 °C
18900 psi
@Temperature -40.0 °F
ASTM Test
 130 MPa
@Temperature -40.0 °C
18900 psi
@Temperature -40.0 °F
ISO Data
Tensile Strength, Yield 88.0 MPa12800 psi50mm/min; ISO 527
 90.0 MPa13100 psi2 in/min; ASTM Test
 30.0 MPa
@Temperature 120 °C
4350 psi
@Temperature 248 °F
ASTM Test
 30.0 MPa
@Temperature 120 °C
4350 psi
@Temperature 248 °F
ISO Data
 40.0 MPa
@Temperature 80.0 °C
5800 psi
@Temperature 176 °F
ISO Data
 40.0 MPa
@Temperature 80.0 °C
5800 psi
@Temperature 176 °F
ASTM Test
 137 MPa
@Temperature -40.0 °C
19900 psi
@Temperature -40.0 °F
ASTM Test
 137 MPa
@Temperature -40.0 °C
19900 psi
@Temperature -40.0 °F
ISO Data
Elongation at Break 7.0 %7.0 %50mm/min, Nominal strain; ISO 527
 12 %12 %2 in/min; ASTM Test
 >= 100 %>= 100 %
 5.0 %
@Temperature -40.0 °C
5.0 %
@Temperature -40.0 °F
ASTM Test
 5.0 %
@Temperature -40.0 °C
5.0 %
@Temperature -40.0 °F
ISO Data
 >= 100 %
@Temperature 120 °C
>= 100 %
@Temperature 248 °F
ISO Data
 >= 100 %
@Temperature 80.0 °C
>= 100 %
@Temperature 176 °F
ISO Data
 >= 100 %
@Temperature 120 °C
>= 100 %
@Temperature 248 °F
ASTM Test
Elongation at Yield 4.0 %4.0 %50mm/min; ISO 527
 4.0 %4.0 %2 in/min; ASTM Test
 3.0 %
@Temperature -40.0 °C
3.0 %
@Temperature -40.0 °F
ASTM Test
 3.0 %
@Temperature -40.0 °C
3.0 %
@Temperature -40.0 °F
ISO Data
 25 %
@Temperature 80.0 °C
25 %
@Temperature 176 °F
ASTM Test
 25 %
@Temperature 80.0 °C
25 %
@Temperature 176 °F
ISO Data
 27 %
@Temperature 120 °C
27 %
@Temperature 248 °F
ASTM Test
 27 %
@Temperature 120 °C
27 %
@Temperature 248 °F
ISO Data
Tensile Modulus 3.70 GPa537 ksi1mm/min; ISO 527
 0.550 GPa
@Temperature 120 °C
79.8 ksi
@Temperature 248 °F
ISO Data
 0.750 GPa
@Temperature 80.0 °C
109 ksi
@Temperature 176 °F
ISO Data
 4.09 GPa
@Temperature -40.0 °C
593 ksi
@Temperature -40.0 °F
ISO Data
Flexural Strength 95.0 MPa13800 psiISO Data
 110 MPa16000 psiASTM Test
 21.0 MPa
@Temperature 120 °C
3050 psi
@Temperature 248 °F
ASTM Test
 30.0 MPa
@Temperature 65.0 °C
4350 psi
@Temperature 149 °F
ASTM Test
 183 MPa
@Temperature -40.0 °C
26500 psi
@Temperature -40.0 °F
ASTM Test
Flexural Modulus 2.80 GPa406 ksiISO Data
 3.17 GPa460 ksiASTM Test
 0.385 GPa
@Temperature 120 °C
55.8 ksi
@Temperature 248 °F
ASTM Test
 0.440 GPa
@Temperature 93.0 °C
63.8 ksi
@Temperature 199 °F
ASTM Test
 0.600 GPa
@Temperature 65.0 °C
87.0 ksi
@Temperature 149 °F
ASTM Test
Izod Impact, Notched 0.320 J/cm
@Temperature -40.0 °C
0.599 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 0.480 J/cm
@Thickness 3.17 mm
0.899 ft-lb/in
@Thickness 0.125 in
ASTM Test
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 81.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
45.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 165 °C329 °FISO 75
 190 °C374 °FASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75
 75.0 °C167 °FASTM Test
Flammability, UL94  V-2
@Thickness 0.700 mm
V-2
@Thickness 0.0276 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection molding
Mold Temperature 80.0 °C176 °FInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8202C PA6 (Conditioned)
BASF Ultramid® A3K PA66 (Dry)
BASF Ultramid® 8202 PA6 (Dry)
BASF Ultramid® 8253 HS PA6 (Dry)
Avient Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)

PBASF9145 / 84909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.