MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Tra-Con Tra-Duct 2960 Snap Cure Electrically Conductive Silver-Filled Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive; Filled/Reinforced Thermoset

Material Notes: TRA-DUCT 2960 is a one or two-part, specially refined and processed silver filled adhesive for high speed manufacturing. Recommended for the microelectronic, automotive computer and telecommunications assembly and packaging industries. TRA-DUCT 2960 provides high electrical and thermal conductivity , along with excellent adhesion to numerous substrate materials. Ideal for chip/die bonding or heat sink attach, TRA-DUCT 2960 snap cures in 2 minutes at 150°C and can withstand operating temperatures up to 175°C. TRA-DUCT 2960 was designed for high speed component attachment of electronic modules, printed circuit board assembly and high frequency shielding, when screen printing or automatic dispensing is desired.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.76 g/cc2.76 g/ccMixed
Volatile Organic Compounds (VOC) Content 5.73 g/l5.73 g/l
Water Absorption 0.12 %0.12 %After 24 hours
Viscosity 144000 cP
@Temperature 25.0 °C
144000 cP
@Temperature 77.0 °F
Mixed (sp #7, 10 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Adhesive Bond Strength 11.0 MPa1600 psiLap shear, alum to alum, 15 min @ 100°C
 13.1 MPa1900 psiLap shear, alum to alum, 2 min @ 150°C
 14.5 MPa2100 psiLap shear, alum to alum, 5 min @ 125°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.00090 ohm-cm0.00090 ohm-cmcured 2 min @ 150°C
 0.0050 ohm-cm0.0050 ohm-cmcured 5 min @ 125°C
 0.0070 ohm-cm0.0070 ohm-cmcured 15 min @ 100°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.5 µm/m-°C25.8 µin/in-°FBelow Tg
 280 µm/m-°C156 µin/in-°FAbove Tg
Thermal Conductivity 1.32 W/m-K9.16 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 175 °C347 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 49.0 °C120 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  2.00 min
@Temperature 150 °C
0.0333 hour
@Temperature 302 °F
 5.00 min
@Temperature 125 °C
0.0833 hour
@Temperature 257 °F
 15.0 min
@Temperature 100 °C
0.250 hour
@Temperature 212 °F
Pot Life 300 min300 min25 grams
Working Life 480 min480 min25 grams
 
Descriptive Properties
Color Silver
Outgassing, NASA Passes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 293-14 Electrically Conductive Silver-Filled Epoxy Adhesive
Abatron 8602-2 A/B Carbon-Filled Electrically Conductive Epoxy Compound
Tra-Con Tra-Duct 916H01 Electronically Conductive Silver-Filled Epoxy
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive
Tra-Con Tra-Duct 8205 One-Part Electrically Conductive Silver-Filled Epoxy

PTRAC094 / 71022

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.