MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Adsyl™ 5 C 30 F Polyolefin
Categories: Polymer; Film; Thermoplastic; Polyolefin; Polyolefin, Film Grade; Polyolefin, Film Grade (Polyolefin)

Material Notes: Description: Adsyl™ 5 C 30 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity and gloss, a low haze, a wide hot-tack range and a Seal-Initiation Temperature (SIT) of 106°C measured on 30 µm film. It does not contain any slip nor anti-blocking agents and is therefore suitable for the production of metallized film. Adsyl™ 5 C 30 F can be processed on both stenter and double bubble equipment. The composition of the product complies with FDA norms and with regulations in force in major European concerning food contact applications.

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ISO 1183
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Heat Seal Strength Initiation Temperature 106.1 °C223.0 °F1.2 mil
 
Thermal PropertiesMetricEnglishComments
Melting Point 135 °C275 °FMTM 15902
 
Optical PropertiesMetricEnglishComments
Haze 1.5 %
@Thickness 0.0500 mm
1.5 %
@Thickness 0.00197 in
MTM 17301, film
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Adsyl™ 3 C 30 F HP Polypropylene Copolymer
LyondellBasell Adsyl 7641 XCP Polypropylene terpolymer
LyondellBasell Adsyl™ 3 C 37 F HP Polypropylene Copolymer
LyondellBasell Adsyl 7572 XCP Polyolefin
LyondellBasell Clyrell RC 211M Polypropylene

PMO765 / 53754

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.