MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 826H01 Thermally Conductive Electrically Insulating Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-BOND 826H01 is a thermally conductive epoxy system that features a small particle size, spherical filler. This filler makes TRA-BOND 826H01 well suited to applications where extrusion through small-gauge needles is desired. TRA-BOND 826H01 is ideal for die and heat sink attach, staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards. This two-part adhesive develops strong, durable, high-impact bonds at room temperature which improves heat transfer while maintaining electrical insulation. TRA-BOND 826H01 bonds readily to itself, and to metals, silica, steatite, alumina, sapphire and other ceramics, glass, plastics and many other materials, because its coefficient of thermal expansion provides a good match for those materials over a fairly wide temperature range. When fully cured, TRA-BOND 826H01 provides excellent resistance to salt solutions, mild acids and alkalis, and many other chemicals including petroleum solvents, lubricating oils and alcohol.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.08 g/cc2.08 g/ccCured
Viscosity 25000 cP25000 cPMixed (cp #52, 20 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80802 hrs @ 65°C
Tensile Strength, Yield 25.68 MPa3725 psi
Adhesive Bond Strength 24.1 MPa3500 psiLap shear, alum to alum, 2 hrs @ 65°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 42.0 µm/m-°C
@Temperature 20.0 °C
23.3 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.895 W/m-K6.21 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 62.0 °C144 °FUltimate Tg; TMA
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 240 min
@Temperature 65.0 °C
2.00 - 4.00 hour
@Temperature 149 °F
 1440 - 4320 min
@Temperature 25.0 °C
24.0 - 72.0 hour
@Temperature 77.0 °F
Working Life 180 min
@Temperature 25.0 °C
180 min
@Temperature 77.0 °F
 
Descriptive Properties
Color Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 826H02 Thermally Conductive Electrically Insulating Compound
Tra-Con Supertherm 816H01 Thermally Conductive Electrically Insulating Compound
Titanium Ti-6Al-4V (Grade 5), Annealed
Armstrong A-12 Epoxy Adhesive, at 2:3 Mix Ratio
Titanium Ti-6Al-4V (Grade 5), Annealed Bar

PTRAC168 / 71096

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.