MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos G50-100 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding physical performance. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: Sheet extrusion, thermoforming and large part blow molding
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D4883
High Load Melt Index 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength at Break 30.3 MPa4400 psi2 in/min.; ASTM D638
Tensile Strength, Yield 26.2 MPa3800 psi2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 800 %>= 800 %2 in/min (50 mm/min); ASTM D-638
Modulus of Elasticity 0.931 GPa135 ksiASTM D638
Flexural Modulus 1.205 GPa174.8 ksiTangent-Method 1; ASTM D790
Tensile Impact Strength 525 kJ/m²250 ft-lb/in²Type L, ASTM D1822
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 µm/m-°C
@Temperature 20.0 °C
66.7 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM D648
Vicat Softening Point 130 °C266 °FASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
processBlow Molding
 Sheet Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis HK060AE Polypropylene Homopolymer
BASF Procom® D 1189 Polypropylene
BASF Procom® D 1188 Polypropylene
Borealis RA130E-6034 Polypropylene Random Copolymer
Borealis Daplen™ ED230HP Polypropylene TPO Compound

PSOLJ9 / 68179

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.