MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oriented Strand Board (OSB), Aspen
Categories: Wood and Natural Products; Wood

Material Notes: OSB is a three particleboard layer composite composed of relatively large, thin, flat wood pieces (strands) bound by a polymeric resin. The two outer surface layers have the strands parallel to the surface. The inner layer has the strands perpendicular - resulting in good mechanical properties for the layered final product. Data is based on small, clear, air-dried samples unless specified.

Key Words: Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 0.800 MPa116 psiPerpendicular
Modulus of Rupture 0.0500 GPa7.25 ksiStatic Bending
Flexural Modulus 7.00 GPa1020 ksiStatic Bending

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Douglas-fir Plywood
Plywood
Carbon-Core 25 mm+2.7 mm Lauan both sides Luan/Meranti Plywood Panels
Flakeboard
ArcelorMittal 01 High formability steel for drawing, Cold rolled

PTSPLY00 / 71377

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.