MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE
Categories: Polymer; Thermoplastic

Material Notes: Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electrical conductivity is needed. Very popular material for valve seats and stem bushings in oil and gas valves and in compressor components.

Information provided by distributor TriStar Plastics Corp.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.96 g/cc0.0708 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565
Tensile Strength, Yield 10.3 MPa1500 psi
Elongation at Break 40 %40 %
Tensile Modulus 1.38 GPa200 ksi
Compressive Yield Strength 12.9 MPa
@Strain 10 %
1870 psi
@Strain 10 %
Izod Impact, Notched 2.94 J/cm5.50 ft-lb/in
Coefficient of Friction, Static 0.0300.030Dry vs. Steel
Limiting Pressure Velocity 0.350 MPa-m/sec10000 psi-ft/min
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 400 ohm400 ohm
Dielectric Constant 2.55
@Frequency 1e+6 Hz
2.55
@Frequency 1e+6 Hz
Dielectric Strength 13.8 kV/mm350 kV/inShort Term
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 288 °C550 °FContinuous
 316 °C600 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °F
Minimum Service Temperature, Air -240 °C-400 °FEmbrittlement Temp
Flammability, UL94 V-0V-0
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Rulon® 125 Bearing/Seal PTFE
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene
Adamas Adalon® 113 PTFE, 23/2% Carbon/Graphite Filled
Saint-Gobain Rulon® AR Bearing/Seal PTFE
Westlake Plastics Zelux® CN-SS Polycarbonate (conductive)

PSTGQ992d / 170604

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.