MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 216E02 Encapsulant for "Fill" Applications
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 216E02 is a two-part epoxy adhesive developed specifically for underfill and encapsulating applications where the combination of excellent mechanical, thermal and electrical properties are required. TRA-BOND 216E02 works in concert with 216E01 to perform `dam` and `fill` functions. TRA-BOND 216E02 exhibits superior adhesion to glass, ceramics, metals, plastics and other electronic materials. Fully cured TRA-BOND 216E02 is an excellent electrical insulator and provides resistance to water, gases and vapors, acids, alkalis, salt solutions, petroleum products and other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/cc
Water Absorption 0.080 %0.080 %
Viscosity 66000 cP
@Temperature 25.0 °C
66000 cP
@Temperature 77.0 °F
Mixed (rv #7, 10 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8989
Adhesive Bond Strength 15.9 MPa2300 psiLap shear, alum to alum, 4 hrs @ 65°C
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 63.0 °C145 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 4320 min
@Temperature 25.0 °C
72.0 hour
@Temperature 77.0 °F
Pot Life 180 min180 min40 grams
Working Life 480 min480 min40 grams
 
Descriptive Properties
Color Black
Mix Ratio, parts by weight100/48.5Resin/Hardener
Thixotropic Index 1.81 rpm/10 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond F202 Spectrally Transparent High Temperature Epoxy Adhesive

PTRAC049 / 70977

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.