MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Riteflex® 663 TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Riteflex 663 is a nominal 63 Shore D thermoplastic polyester elastomer with medium modulus.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D792
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Water Absorption 0.30 %
@Temperature 22.8 °C
0.30 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.017 - 0.020 cm/cm0.017 - 0.020 in/inISO 294-4
 0.019 cm/cm0.019 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.017 - 0.021 cm/cm0.017 - 0.021 in/inISO 294-4
Melt Flow 16 g/10 min16 g/10 minASTM D1238
 19 g/10 min
@Load 2.16 kg,
Temperature 240 °C
19 g/10 min
@Load 4.76 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
 636315 sec; ISO 868
 6363ISO 868
Tensile Strength at Break 26.2 MPa3800 psiASTM D638
 38.0 MPa5510 psi50mm/min; ISO 527-2/1A
 38.0 MPa5510 psiISO 527-1/2
Tensile Strength, Yield 22.0 MPa3190 psi50mm/min; ISO 527-2/1A
Tensile Stress at Strain  13.0 MPa
@Strain 5.0 %
1890 psi
@Strain 5.0 %
ISO 527-1/2
 18.0 MPa
@Strain 10 %
2610 psi
@Strain 10 %
ISO 527-1/2
 19.0 MPa
@Strain 50 %
2760 psi
@Strain 50 %
ISO 727-1/2
 21.0 MPa
@Strain 50 %
3050 psi
@Strain 50 %
ISO 527-2/1A
Elongation at Break >= 50 %>= 50 %
 320 %320 %ASTM D638
Elongation at Yield 44 %44 %50mm/min; ISO 527-2/1A
Tensile Modulus 0.350 GPa50.8 ksi50mm/min; ISO 527-2/1A
 0.365 GPa52.9 ksiASTM D638
Flexural Strength 17.5 MPa2540 psiISO 178
Flexural Modulus 0.325 GPa47.1 ksiISO 178
 0.325 GPa47.2 ksiASTM D790
 1.564 GPa
@Temperature -40.0 °C
226.8 ksi
@Temperature -40.0 °F
ASTM D790
 1.90 GPa
@Temperature -40.0 °C
276 ksi
@Temperature -40.0 °F
ISO 178
Resilience 4040Bayshore, %; ASTM D2632
 4040Bayshore, %
Flex Crack Resistance >= 1.00e+6>= 1.00e+6Ross flex
Izod Impact, Notched NBNBASTM D256
 0.267 J/cm
@Temperature -40.0 °C
0.500 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180
 74.0 kJ/m²35.2 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 10.5 J/cm²50.0 ft-lb/in²partial break; ISO 179/1eA
 2.20 J/cm²
@Temperature -30.0 °C
10.5 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Tear Strength 160 kN/m913 pliISO 34-1
 266 kN/m1520 pliASTM D624
 270 kN/m1540 pliASTM D1004
Compression Set <= 1.0 %<= 1.0 %ASTM D395
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+13 ohm-cm2.00e+13 ohm-cmASTM D257
 2.00e+15 ohm-cm2.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 13.4 kV/mm340 kV/inshort term; ASTM D149
 14.0 kV/mm356 kV/inIEC 60243-1
Dissipation Factor 0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VASTM D3638
 >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 180 µm/m-°C100 µin/in-°FISO 11359-2
Melting Point 210 °C410 °FASTM D3418
 212 °C414 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 114 °C237 °FISO 75-1, -2
Vicat Softening Point 195 °C383 °FASTM D1525
Glass Transition Temp, Tg -42.8 °C-45.0 °FASTM D3418
Flammability, UL94 HBHB
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 55.0 °C68.0 - 131 °Fcavity
 215 - 235 °C419 - 455 °Fhot runner
Feed Temperature 200 - 215 °C392 - 419 °F
Zone 1 200 - 215 °C392 - 419 °F
Zone 2 215 - 230 °C419 - 446 °F
Zone 3 215 - 230 °C419 - 446 °F
Zone 4 215 - 235 °C419 - 455 °F
Die Temperature 215 - 235 °C419 - 455 °F
Melt Temperature 215 - 235 °C419 - 455 °F
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 4.00 hour4.00 hour
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Riteflex® 655A TPC, Unfilled
Celanese Riteflex® 672 TPC, Unfilled
Celanese Riteflex® 640A TPC, Unfilled
Celanese Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
Celanese Riteflex® 663HS TPC, Unfilled

PHCQ454 / 178909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.