MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel UREA 25.22.2 Plants
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Description: CLI UREA 25.22.2 chemical composition has been optimized for specific uses in Urea plants. It is a 310L modified austenitic stainless steel with low carbon, low silicon and high nitrogen additions in order to stabilize and strengthen the austenitic phase. The alloy is designed to obtain a fully austenitic stainless steel free of intermetallic phases as intergranular carbide precipitations which affects the corrosion resistance properties of the alloy in urea containing solutions. The ferrite level is kept under 0.5% in the solution annealing and water quenched conditions. The alloy is particularly designed for improved corrosion resistance properties in urea carbonate environments including strippers. The grade is also well designed for resistance in wet corrosive conditions due to its high contents of chromium, molybdenum and nitrogen (PREN = 33)

Information provided by manufacturer.

Key Words: EN 10028-7 X1 Cr Ni Mo N 25.22.2 - 1.4466, AFNOR Z2 CND 25.22.AZ, DIN W.Nr 1.4466 / 1.4465, ASTM 310 Mo LN
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.90 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 550 MPa79800 psiTypical after Solution Annealing
Tensile Strength, Yield  260 MPa
@Strain 0.2 %
37700 psi
@Strain 0.2 %
Typical after Solution Annealing
 290 MPa
@Strain 1 %
42100 psi
@Strain 1 %
Typical after Solution Annealing
Elongation at Break 40 %40 %Typical
Modulus of Elasticity 200 GPa29000 ksi
Poissons Ratio 0.3330.333Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
10900 ksi
@Temperature 68.0 °F
Charpy Impact >= 120 J>= 88.5 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000950 ohm-cm
@Temperature 20.0 °C
0.0000950 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.0 µm/m-°C
@Temperature 20.0 - 100 °C
8.89 µin/in-°F
@Temperature 68.0 - 212 °F
 16.5 µm/m-°C
@Temperature 20.0 - 300 °C
9.17 µin/in-°F
@Temperature 68.0 - 572 °F
 17.5 µm/m-°C
@Temperature 20.0 - 500 °C
9.72 µin/in-°F
@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 °C
0.120 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
97.2 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 25 %25 %
Iron, Fe 48.36 - 50.78 %48.36 - 50.78 %As remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 2.1 %2.1 %
Nickel, Ni 22 %22 %
Nitrogen, N 0.12 %0.12 %
Silicon, Si <= 0.40 %<= 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants
310 Stainless Steel, annealed sheet
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel
Industeel VIRGO 39 16% Cr, 5% Ni, Martensitic Stainless Steel
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel

NINDUST37 / 17575

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.