MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Paxon™ BU46-060 High Density Polyethylene (HDPE), Copolymer Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Copolymer Film Grade

Material Notes: BU46-060 is a high molecular weight high density polyethylene copolymer which contains a UV inhibitor.  It possesses a combination of excellent processability, outstanding melt strength, high impact strength, chemical resistance, and high stress cracking resistance. 

Availability:  Latin America, North America.  Applications: intermediate bulk containers.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ASTM D4883
ESCR 100% Igepal® >= 1000 hour>= 1000 hourASTM D1693
Melt Flow <= 0.10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
<= 0.10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 6.3 g/10 min
@Load 21.6 kg,
Temperature 190 °C
6.3 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.8 MPa3300 psiASTM D638
Flexural Modulus, 1% Secant 1030 MPa150000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 124 °C255 °FASTM D1525
Brittleness Temperature <= -76.1 °C<= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Alathon® L5005V High Density Polyethylene, HMW Film Grade
Formosa Plastics Formolene® HP4401 Pipe HDPE
ExxonMobil Paxon™ 7003 Crosslinkable Rotational Molding Resin
Aluminum 6061-T4; 6061-T451
Total Finathene® 3344N Natural HDPE pipe grade

PEX98891 / 238273

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.