MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow BETAFOAM™ 89100/89120
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: BETAFOAM™ 89100/89120 is a low-density, all-water blown rigid polyurethane foam. The components were engineered to produce a foam for providing barrier protection against airborne noise. Foam is produced by the rapid mixing of both components under high shear conditions. These components were formulated for fast reaction and high volume expansion. The foam has adhesion to primed metal surfaces.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0320 g/cc0.00116 lb/in³Free Rise Density (Cured)
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength >= 0.0414 MPa>= 6.00 psi
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.00 %0.00 %20 min after foam manufacture
 0.40 %
@Temperature 37.8 °C,
Time 605000 sec
0.40 %
@Temperature 100 °F,
Time 168 hour
 2.4 %
@Temperature 121 °C,
Time 86400 sec
2.4 %
@Temperature 250 °F,
Time 24.0 hour
24 hrs @ 250°F
 
Descriptive Properties
Aged Weight Loss %1.924 hrs @ 175°F
Volume Expansion %, min3400Cured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow BETAFOAM™ 87100/87120
Dow BETAFOAM™ 87100/87156
Dow BETAFOAM™ 87100/87155
Dow BETAFOAM™ 87100/87124
Dow BETAFOAM™ 89120 Water/Amine catalyst

PDOW1126 / 30330

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.