MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kinetics MIM 2.5% SiFe Soft Magnetic Steel
Categories: Metal; Electronic/Magnetic Alloy; Ferrous Metal

Material Notes: Low alloy steel, silicon. A work hardenable steel alloy that offers very good magnetic properties, tensile strength, hardness, wear resistance, and increased spring steel strength. Can be plated or coated for corrosion resistance. Often used for armatures, relays, solenoids, and applications where good magnetic, low core loss and high electrical resistivity in AC and DC applications is required.

Property values reported are typical for Kinetics' MIM products.

Metal Injection Molding General Notes: Fine metal powders (generally <25 microns in diameter) are combined with a polymer binder system to form a feedstock suitable for injection molding. Kinetics' feedstock is compounded using specific binder and metal powder formulations to control consistency, quality, and dimensional repeatability of parts produced. While standard plastic injection molding machines and molds are used to produce MIM parts, due to the presence of the polymer binder in MIM feedstocks, mold cavities are designed approximately 20% larger than the final part size. Like plastics, MIM molds may have multiple cavities, inserts, slides, unscrewing cores, and hot runner systems. After molding, green parts are debound and sintered at temperatures up to 2,600°F. During debinding, the polymer binder breaks down and dissipates while the metal particles retain all of the molded features. The metal particles fuse together during sintering and the part shrinks approximately 20% to form a solid metal part.

Information provided by Kinetics, Inc.

Key Words: Metal Injection Molding
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.61 g/cc0.275 lb/in³Sintered
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8282
Tensile Strength, Ultimate 483 MPa70000 psi
Tensile Strength, Yield 338 MPa49000 psi
Elongation at Break 24 %24 %in 1 inch
Reduction of Area 43 %43 %
Charpy Impact, Unnotched 213 J157 ft-lb1/2 size bar
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.060 %<= 0.060 %
Iron, Fe 97.19 - 97.85 %97.19 - 97.85 %Iron content calculated by difference.
Silicon, Si 2.15 - 2.75 %2.15 - 2.75 %
 
Descriptive Properties
Surface Finish24 Ra

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kinetics MIM 4605 Low Alloy Steel (Quenched + Tempered)
Kinetics MIM K3 Heat Treat
Kinetics MIM K3 Heat Treat as Sintered
Kinetics MIM F1537 (ASTM F1537) HIP and Heat Treat
PSM Industries PolyAlloys MIM-Fe-%3Si Grade 2 Soft Magnetic Steel

NKINET13 / 17746

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.