MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Formosa Plastics Formolene® HL3812 Film (Hexene) HDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Medium Density Polyethylene

Formolene® HL3812 is a high molecular weight hexene copolymer resin that is tailored specifically for geomembrane applications. The resin provides an excellent balance of ESCR properties, broad fusion range, excellent melt strength and good overall processability

Applications: Landfill Liners, Gasoline and Chemical Tank Containment Liners, Tunnel Moisture Barriers and Mine Tailing Collection Projects

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourSP-NCTL; ASTM D5397
ESCR 100% Igepal® >= 1500 hour>= 1500 hourCondition C, F50; ASTM D1693
ESCR 10% Igepal® >= 1500 hour>= 1500 hourCondition B, F50; ASTM D1693
Melt Flow 0.080 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.080 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 12 g/10 min
@Load 21.6 kg,
Temperature 190 °C
12 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Yield 17.9 MPa2600 psi2" (50mm) per min, Type IV; ASTM D638
Elongation at Break 850 %850 %2" (50mm) per min, Type IV; ASTM D638
Flexural Modulus 0.827 GPa120 ksiTangent – 16:1 span:depth, 0.5 in./min.; ASTM D790
Tensile Impact Strength 504 kJ/m²240 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 59.0 °C138 °FMethod A; ASTM D648
Vicat Softening Point 117 °C243 °FASTM D648
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® HL5010 Blow Molding HDPE
Solder Alloy (UNS L50170)
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
ExxonMobil HD 5451HL High Density Polyethylene Resin
NOVA Chemicals Novapol® HB-W747-A HDPE Extrusion Resin

PFPCPQ052 / 150284

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.