MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Resin Type: enhanced linear low density polyethylene, high antiblock, and processing aid additive

Characteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, can be used straight or blended with LDPE or HDPE, high antiblock

Applications: thick or thin film

Applications where superior toughness and abuse resistance, hot-tack and heat-seal, and optical properties are critical

Recommended processing conditions: 6.35 cm extruder. 24:1 screw L/D ratio. 0.203 cm die opening. Melt temperature 232°C. Blow up ratio 2.5:1. Output rate 8.0 lb/hr/in die cir.

Data provided by Chevron Phillips Chemical Company, LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³Base Resin; ASTM D4833-89
Thickness 25.4 microns1.00 mil
Melt Flow 0.50 g/10 min0.50 g/10 minASTM D1238E
Slip Level 0.000 ppm0.000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 550 %550 %ASTM D882
Film Elongation at Break, TD 690 %690 %ASTM D882
Coefficient of Friction 1.01.0ASTM D1894
Elmendorf Tear Strength, MD 20.9 g/micron530 g/milNotched; ASTM D1922
Elmendorf Tear Strength, TD 31.1 g/micron790 g/milASTM D1992
Film Tensile Strength at Break, MD 51.5 MPa7470 psiASTM D882
Film Tensile Strength at Break, TD 40.7 MPa5900 psiASTM D882
1% Secant Modulus, MD 179 MPa25900 psiASTM D882
1% Secant Modulus, TD 190 MPa27600 psiASTM D882
Hot Tack Strength, Ultimate 3.80 N0.854 lb (f)
Hot Tack Initiation Temperature 86.1 °C187 °Fat 0.5N; ASTM D3706
Heat Seal Strength, Ultimate 13.6 N3.06 lb (f)
Heat Seal Strength Initiation Temperature 96.1 °C205 °Fat 0.5 lb.
 
Optical PropertiesMetricEnglishComments
Haze 14 %14 %ASTM D2457
Gloss 54 %54 %45°; ASTM D2457
 87 %87 %60°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 232 °C450 °F
Die Opening 0.203 cm0.0799 in
Extruder Size 6.35 cm2.50 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 222B Polyethylene Film Grade
Borealis FG5190 Linear Low Density Polyethylene
Borealis FG5224 Linear Low Density Polyethylene
Chevron Phillips Vytek™ V205A Enhanced LLDPE Blown Film Resin
Borealis FG5199 Linear Low Density Polyethylene

PCHEVVY7 / 20585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.