MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Potters Industries Spheriglass® 2024 Solid Glass Spheres
Categories: Ceramic; Glass; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:
  • Low Uniform Shrinkage
  • Low Warpage
  • High Flexural Modulus
  • High Abrasion Resistance
  • High Compressive Strength
  • Increased Surface Hardness
  • Better Stress Distribution

These and other characteristics enable the spheres to be used in a wide range of applications in the automotive, chemical, electronic, industrial, engineering, and photographic industries.

Information provided by Potters Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.50 g/cc2.50 g/cc
Bulk Density 1.46 g/cc0.0527 lb/in³Untapped; ASTM D 3101-78
 1.57 g/cc0.0567 lb/in³Tapped; ASTM D 3101-78
Oil Absorption 18 %18 %ASTM D1483
Particle Size 106 - 212 µm106 - 212 µmRange
Particle Mesh Size 70 - 140 Mesh70 - 140 Mesh
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 6.06.0
Modulus of Elasticity 68.9 GPa10000 ksi
Poissons Ratio 0.160.16Calculated
Shear Modulus 29.6 GPa4300 ksi
Coefficient of Friction 0.90 - 1.00.90 - 1.0
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.50e+12 ohm-cm6.50e+12 ohm-cm
Dielectric Constant 6.9
@Frequency 1e+6 Hz
6.9
@Frequency 1e+6 Hz
Dissipation Factor 0.0085
@Frequency 1e+6 Hz
0.0085
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 °C
5.00 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.51 W/m-K
@Temperature 500 °C
10.4 BTU-in/hr-ft²-°F
@Temperature 932 °F
Softening Point 704 °C1300 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.40 %0.40 %
CaO 9.8 %9.8 %
Fe2O3 0.20 %0.20 %
Free Iron <= 0.10 %<= 0.10 %
K2O 0.10 %0.10 %
MgO 3.3 %3.3 %
Na2O 13.7 %13.7 %
SiO2 72.5 %72.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Potters Industries Spheriglass® 2530 Solid Glass Spheres
Aluminum 2024-T3
Potters Industries Spheriglass® 3000 Solid Glass Spheres
Aluminum 2024-T4; 2024-T351 (Included Extended Size/Shape Data)
Aluminum 2024-T6

CPOT00_b / 147475

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.