MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® Redux® 340U(SP) (0.01 psf) Modified epoxy film adhesive for bonding metallic and composite components
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux® 340U(SP) is a high temperature modified epoxy film adhesive curing at 175°C (350°F). It was developed as a low weight film adhesive for space applications. It is suitable for bonding metal to metal, where operating temperatures are experienced up to 200°C (392°F) for short periods, or 180°C (356°F) for continuous operation. Redux® 340U(SP) is a hot melt film which is free from solvents and consequently has a very low volatile content.

Features: Cures in 1 hour at 175°C (350°F); Good hot lap shear performance up to 180°C(356°F); Excellent metal-metal peel properties; Excellent drape and handleability; Good reticulating characteristics; very low volatile content and low outgassing properties; Only available un-supported.
Applications: Metal to metal bonding; Composite to composite bonding; Space applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Outgassing - Total Mass Loss 0.109 %0.109 %Recovered Mass Loss (RML), Typical result; ESA PSS-01-702
 1.168 %1.168 %Total Mass Loss (TML), Typical result; ESA PSS-01-702
Collected Volatile Condensable Material 0.00 %0.00 %ESA PSS-01-702
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  18.0 MPa
@Temperature 150 °C
2610 psi
@Temperature 302 °F
Lap Shear
 30.99 MPa
@Temperature 22.2 °C
4495 psi
@Temperature 72.0 °F
Lap Shear
Peel Strength 5.35 kN/m
@Temperature 22.2 °C
30.5 pli
@Temperature 72.0 °F
Floating Roller Peel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F
 200 °C392 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month
@Temperature -17.8 °C
18.0 Month
@Temperature 0.000 °F
 
Descriptive Properties
Roll Width (in)47.2
Standard Roll (ft2)538

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® Redux® 609 (0.04 psf) Adhesive film for bonding metallic and composite components
Hexcel® Redux® 382H (0.03 psf) Film Adhesive
Hexcel® Redux® 335U Adhesive film for bonding metallic and composite components (0.03 psf)
Hexcel® Redux® 322U Modified epoxy film adhesive (0.06 psf)
Hexcel® Redux® 312 Modified epoxy film adhesive (0.06 psf)

PHEXC461 / 99280

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.