MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese VECTRAN™ V300P Co-Extrudable Liquid Crystal Polymer (LCP)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Unfilled

Material Notes: Description: PRELIMINARY DATA SHEET: Co-extrudable LCP for Barrier Applications. Vectran V300P Liquid Crystal Polymer is characterized by its low processing temperature, excellent barrier properties independent of relative humidity, chemical resistance and contact clarity in thin film applications. This material is not suitable for medical or dental implants.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.040 %0.040 %at 50% RH; ISO 62
Moisture Vapor Transmission 0.0157 cc-mm/m²-24hr-atm0.0400 cc-mil/100 in²-24hr-atmat 38°C; DIN 53122-2
Oxygen Transmission 0.0394 cc-mm/m²-24hr-atm0.100 cc-mil/100 in²-24hr-atm73°F, 100%RH; DIN 53380 part 3
 0.0472 cc-mm/m²-24hr-atm0.120 cc-mil/100 in²-24hr-atm73°F, 0% RH; DIN 53380 part 3
Carbon Dioxide Transmission 0.0945 cc-mm/m²-24hr-atm0.240 cc-mil/100 in²-24hr-atm25°C, 100% RH; ISO/CD 15105-2C
Melt Flow 18 g/10 min
@Temperature 230 °C
18 g/10 min
@Temperature 446 °F
I2, nominal
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 153 MPa22200 psi5 mm/min; ISO 527-2/1A
Elongation at Break 2.4 %2.4 %5 mm/min; ISO 527-2/1A
Tensile Modulus 11.5 GPa1670 ksi1 mm/min; ISO 527-2/1A
Flexural Strength 178 MPa25800 psiISO 178
Flexural Modulus 9.70 GPa1410 ksiISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 44.0 kJ/m²20.9 ft-lb/in²ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FISO 75-1, -2
Glass Transition Temp, Tg 110 °C230 °FISO 3146
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 185 - 195 °C365 - 383 °F
Middle Barrel Temperature 205 - 215 °C401 - 419 °F
Front Barrel Temperature 225 - 235 °C437 - 455 °F
Die Temperature 225 - 235 °C437 - 455 °F
Melt Temperature 225 - 235 °C437 - 455 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRAN™ V400P Co-Extrudable Liquid Crystal Polymer (LCP)
Celanese VECTRAN™ V100P Co-Extrudable Liquid Crystal Polymer (LCP)
Celanese VECTRAN™ V200P Co-Extrudable Liquid Crystal Polymer (LCP)
Kuraray Vectran® HT 1500/300 LCP Fiber
Kuraray Vectran® NT 1500/300 LCP Fiber

PHCV58 / 45899

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.