Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength, Yield | 2.965 MPa @Temperature 93.0 °C | 430.0 psi @Temperature 199 °F |
| 3.896 MPa @Temperature 93.0 °C | 565.1 psi @Temperature 199 °F |
| 4.682 MPa @Temperature -59.0 °C | 679.1 psi @Temperature -74.2 °F |
| 4.806 MPa @Temperature 24.0 °C | 697.1 psi @Temperature 75.2 °F |
| 419 MPa @Temperature 71.0 °C | 60800 psi @Temperature 160 °F |
| 420 MPa @Temperature 93.0 °C | 60900 psi @Temperature 199 °F |
| 462 MPa @Temperature 71.0 °C | 67000 psi @Temperature 160 °F |
| 485 MPa @Temperature -54.0 °C | 70300 psi @Temperature -65.2 °F |
| 637 MPa @Temperature 24.0 °C | 92400 psi @Temperature 75.2 °F |
Tensile Modulus | 49.6 GPa @Temperature 71.0 °C | 7190 ksi @Temperature 160 °F |
| 51.7 GPa @Temperature 71.0 °C | 7500 ksi @Temperature 160 °F |
| 53.8 GPa @Temperature 93.0 °C | 7800 ksi @Temperature 199 °F |
| 55.2 GPa @Temperature -54.0 °C | 8010 ksi @Temperature -65.2 °F |
| 56.5 GPa @Temperature 24.0 °C | 8190 ksi @Temperature 75.2 °F |
Compressive Yield Strength | 410 MPa @Temperature 71.0 °C | 59500 psi @Temperature 160 °F |
| 469 MPa @Temperature 93.0 °C | 68000 psi @Temperature 199 °F |
| 536 MPa @Temperature 71.0 °C | 77700 psi @Temperature 160 °F |
| 627 MPa @Temperature 24.0 °C | 90900 psi @Temperature 75.2 °F |
| 745 MPa @Temperature -59.0 °C | 108000 psi @Temperature -74.2 °F |
Compressive Modulus | 44.8 GPa @Temperature 71.0 °C | 6500 ksi @Temperature 160 °F |
| 46.9 GPa @Temperature 93.0 °C | 6800 ksi @Temperature 199 °F |
| 48.3 GPa @Temperature 71.0 °C | 7010 ksi @Temperature 160 °F |
| 50.3 GPa @Temperature -59.0 °C | 7300 ksi @Temperature -74.2 °F |
| 51.0 GPa @Temperature 24.0 °C | 7400 ksi @Temperature 75.2 °F |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding