System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
;
Polycarbonate (PC)
Material Notes:
Description: Injection Molding, PC/ABS, Flame Retardance, Heat Resistance
Application: E&E (Housing)
CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.18
g/cc
1.18
g/cc
ASTM D792
Maximum Moisture Content
0.020
0.020
Injection Molding
Linear Mold Shrinkage, Flow
0.0040
-
0.0060
cm/cm
@Thickness 3.20 mm
0.0040
-
0.0060
in/in
@Thickness 0.126 in
ASTM D955
Melt Flow
5.0
g/10 min
@Load 2.16 kg,
Temperature 250 °C
5.0
g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
113
113
ASTM D785
Tensile Strength, Yield
53.9
MPa
@Thickness 3.20 mm
7820
psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break
50 %
@Thickness 3.20 mm
50 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength
82.4
MPa
@Thickness 3.20 mm
11900
psi
@Thickness 0.126 in
10mm/min; ASTM D790
Flexural Modulus
2.35
GPa
@Thickness 3.20 mm
341
ksi
@Thickness 0.126 in
10mm/min; ASTM D790
Izod Impact, Notched
5.88
J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
11.0
ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+11
ohm-cm
1.00e+11
ohm-cm
Dielectric Strength
38.0
kV/mm
965
kV/in
Arc Resistance
60
-
120
sec
60
-
120
sec
ASTM D495
Hot Wire Ignition, HWI
7.0
-
15
sec
@Thickness >=0.820 mm
7.0
-
15
sec
@Thickness >=0.0323 in
7.0
-
15
sec
@Thickness >=1.50 mm
7.0
-
15
sec
@Thickness >=0.0591 in
30
-
60
sec
@Thickness >=3.00 mm
30
-
60
sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI
30
-
60
arcs
@Thickness 0.820 mm
30
-
60
arcs
@Thickness 0.0323 in
>=
120
arcs
@Thickness 1.50 mm
>=
120
arcs
@Thickness 0.0591 in
>=
120
arcs
@Thickness 3.00 mm
>=
120
arcs
@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR
>=
150
mm/min
>=
5.91
in/min
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
112
°C
@Thickness 6.40 mm
234
°F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical
85.0
°C
@Thickness >=0.820 mm
185
°F
@Thickness >=0.0323 in
85.0
°C
@Thickness >=1.50 mm
185
°F
@Thickness >=0.0591 in
85.0
°C
@Thickness >=3.00 mm
185
°F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact
65.0
°C
@Thickness >=0.820 mm
149
°F
@Thickness >=0.0323 in
65.0
°C
@Thickness >=1.50 mm
149
°F
@Thickness >=0.0591 in
65.0
°C
@Thickness >=3.00 mm
149
°F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact
70.0
°C
@Thickness >=0.820 mm
158
°F
@Thickness >=0.0323 in
70.0
°C
@Thickness >=1.50 mm
158
°F
@Thickness >=0.0591 in
70.0
°C
@Thickness >=3.00 mm
158
°F
@Thickness >=0.118 in
Flammability, UL94
V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
5VB
@Thickness >=3.00 mm
5VB
@Thickness >=0.118 in
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
220
-
240
°C
428
-
464
°F
Injection Molding
Middle Barrel Temperature
235
-
255
°C
455
-
491
°F
Injection Molding
Front Barrel Temperature
250
-
265
°C
482
-
509
°F
Injection Molding
Nozzle Temperature
250
-
265
°C
482
-
509
°F
Injection Molding
Melt Temperature
235
-
265
°C
455
-
509
°F
Injection Molding
Mold Temperature
50.0
-
80.0
°C
122
-
176
°F
Injection Molding
Drying Temperature
75.0
-
85.0
°C
167
-
185
°F
Injection Molding
Dry Time
3.00
-
5.00
hour
3.00
-
5.00
hour
Injection Molding
Back Pressure
0.00200
-
0.00600
MPa
0.290
-
0.870
psi
Injection Molding
Screw Speed
40
-
70
rpm
40
-
70
rpm
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
E-Polymers Tekaloy® G70F2 G70NH, Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant
Kingfa JH950-402 Flame Retardant PC/ABS Alloy
E-Polymers Tekaloy® G70NH Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy
Gichem GIBLEND E45X3/VO ABS - Polycarbonate - PC/ABS Flame Retardant
PLAY598 / 148608
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.