MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ Surlyn® 8527 Ionomer Resin, Sodium  (discontinued **)
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Molded

Material Notes: Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neutralization levels for this grade result in excellent clarity and abrasion resistance. The resin can be injection or blow molded, and is processable by extrusion into sheets or shapes. It complies with the provisions of U.S. Food and Drug Administration (FDA) Title 21 Code of Regulations 177:1330 - ionomer resins.

Data provided by the manufacturer.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength, Ultimate 29.0 MPa4210 psiASTM D638
Tensile Strength, Yield 12.4 MPa1800 psi50 mm/min cross speed; ASTM D638
Elongation at Break 450 %450 %ASTM D638
Flexural Modulus 0.220 GPa31.9 ksiASTM D790
Izod Impact, Notched 6.10 J/cm11.4 ft-lb/inASTM D256
Tensile Impact Strength 1160 kJ/m²552 ft-lb/in²ASTM D1822S
Abrasion 600600NBS Index; ASTM D1630
 
Thermal PropertiesMetricEnglishComments
CTE, linear 140 µm/m-°C
@Temperature -20.0 - 32.0 °C
77.8 µin/in-°F
@Temperature -4.00 - 89.6 °F
ASTM D696
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
Melting Point 93.0 °C199 °FDTA
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °C111 °FASTM D648
Vicat Softening Point 73.0 °C163 °FRate B, ASTM D1525-70
Brittleness Temperature -95.0 °C-139 °FASTM D746
Flame Spread 22.9 mm/min0.902 in/minASTM D635
 
Optical PropertiesMetricEnglishComments
Haze 6.0 %
@Thickness 6.35 mm
6.0 %
@Thickness 0.250 in
ASTM D1003A
Gloss 75 %75 %20° per ASTM D523-6

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Surlyn® 1707 Sodium Ionomer
Dow Surlyn® 6320 Magnesium Ionomer
Dow Surlyn® 8150 Ionomer Resin, Sodium
Dow Surlyn® 2601B Sodium Ionomer
Dow Surlyn® 9120 Ionomer Resin, Zinc

PDU407 / 33058

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.