MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Low Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Low Alloy Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.50 - 8.08 g/cc0.271 - 0.292 lb/in³Average value: 7.84 g/cc Grade Count:1765
Particle Size 6.70 - 12.0 µm6.70 - 12.0 µmAverage value: 9.27 µm Grade Count:20
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 121 - 578121 - 578Average value: 274 Grade Count:1311
Hardness, Knoop 140 - 682140 - 682Average value: 307 Grade Count:1261
Hardness, Rockwell B 45.0 - 11245.0 - 112Average value: 96.2 Grade Count:1213
Hardness, Rockwell C 10.0 - 66.010.0 - 66.0Average value: 30.8 Grade Count:1192
Hardness, Vickers 36.0 - 66136.0 - 661Average value: 297 Grade Count:1273
Tensile Strength, Ultimate 180 - 2730 MPa26100 - 396000 psiAverage value: 996 MPa Grade Count:1614
Tensile Strength, Yield 110 - 2400 MPa16000 - 347000 psiAverage value: 715 MPa Grade Count:1612
Elongation at Break 2.00 - 37.0 %2.00 - 37.0 %Average value: 18.6 % Grade Count:1579
Elongation at Yield 1.00 - 40.0 %1.00 - 40.0 %Average value: 16.9 % Grade Count:4
Reduction of Area 3.00 - 75.0 %3.00 - 75.0 %Average value: 53.2 % Grade Count:609
Modulus of Elasticity 183 - 213 GPa26500 - 30900 ksiAverage value: 204 GPa Grade Count:1568
Compressive Yield Strength 1650 - 1800 MPa239000 - 260000 psiAverage value: 1700 MPa Grade Count:12
Bulk Modulus 152 - 170 GPa22000 - 24700 ksiAverage value: 160 GPa Grade Count:1481
Poissons Ratio 0.270 - 0.3000.270 - 0.300Average value: 0.290 Grade Count:1552
Fatigue Strength 138 - 772 MPa20000 - 112000 psiAverage value: 472 MPa Grade Count:17
Fracture Toughness 15.4 - 143 MPa-m½14.0 - 130 ksi-in½Average value: 73.7 MPa-m½ Grade Count:15
Machinability 40.0 - 75.0 %40.0 - 75.0 %Average value: 59.8 % Grade Count:1219
Shear Modulus 70.0 - 82.0 GPa10200 - 11900 ksiAverage value: 79.8 GPa Grade Count:1598
Izod Impact 9.00 - 138 J6.64 - 102 ft-lbAverage value: 57.5 J Grade Count:132
Charpy Impact 15.0 - 339 J11.1 - 250 ft-lbAverage value: 56.3 J Grade Count:15
Charpy Impact, Unnotched 39.3 - 176 J29.0 - 130 ft-lbAverage value: 82.0 J Grade Count:8
Bend Radius, Minimum 0.000 - 4.00 t0.000 - 4.00 tAverage value: 1.65 t Grade Count:101
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.000142 ohm-cm0.00000200 - 0.000142 ohm-cmAverage value: 0.0000222 ohm-cm Grade Count:1471
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.1 - 14.9 µm/m-°C5.61 - 8.28 µin/in-°FAverage value: 12.6 µm/m-°C Grade Count:720
Specific Heat Capacity 0.448 - 0.669 J/g-°C0.107 - 0.160 BTU/lb-°FAverage value: 0.475 J/g-°C Grade Count:1297
Thermal Conductivity 25.3 - 93.0 W/m-K176 - 645 BTU-in/hr-ft²-°FAverage value: 46.5 W/m-K Grade Count:1410
Transformation Temperature 183 - 910 °C361 - 1670 °FAverage value: 600 °C Grade Count:61
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.0100 - 1.20 %0.0100 - 1.20 %Average value: 0.133 % Grade Count:53
Boron, B 0.000500 - 0.00600 %0.000500 - 0.00600 %Average value: 0.00225 % Grade Count:202
Carbon, C 0.0300 - 1.29 %0.0300 - 1.29 %Average value: 0.329 % Grade Count:1749
Chromium, Cr 0.130 - 5.50 %0.130 - 5.50 %Average value: 0.823 % Grade Count:1255
Cobalt, Co 3.75 - 12.0 %3.75 - 12.0 %Average value: 8.35 % Grade Count:31
Copper, Cu 0.100 - 1.50 %0.100 - 1.50 %Average value: 0.493 % Grade Count:113
Hydrogen, H 0.00100 - 0.00250 %0.00100 - 0.00250 %Average value: 0.00200 % Grade Count:3
Iron, Fe 63.0 - 100 %63.0 - 100 %Average value: 96.5 % Grade Count:1798
Manganese, Mn 0.100 - 3.00 %0.100 - 3.00 %Average value: 0.813 % Grade Count:1740
Molybdenum, Mo 0.0600 - 4.80 %0.0600 - 4.80 %Average value: 0.341 % Grade Count:1267
Nb + V 0.0200 - 0.150 %0.0200 - 0.150 %Average value: 0.124 % Grade Count:5
Nickel, Ni 0.100 - 18.5 %0.100 - 18.5 %Average value: 1.88 % Grade Count:946
Niobium, Nb (Columbium, Cb) 0.00500 - 0.150 %0.00500 - 0.150 %Average value: 0.0428 % Grade Count:92
Nitrogen, N 0.00100 - 0.0300 %0.00100 - 0.0300 %Average value: 0.0178 % Grade Count:18
Oxygen, O 0.00250 - 0.100 %0.00250 - 0.100 %Average value: 0.0627 % Grade Count:7
Phosphorus, P 0.00100 - 0.150 %0.00100 - 0.150 %Average value: 0.0330 % Grade Count:1663
Silicon, Si 0.0100 - 2.20 %0.0100 - 2.20 %Average value: 0.285 % Grade Count:1732
Sulfur, S 0.00100 - 0.400 %0.00100 - 0.400 %Average value: 0.0367 % Grade Count:1697
Titanium, Ti 0.0100 - 1.40 %0.0100 - 1.40 %Average value: 0.324 % Grade Count:58
Vanadium, V 0.00500 - 0.300 %0.00500 - 0.300 %Average value: 0.104 % Grade Count:171
Zirconium, Zr 0.0100 - 0.150 %0.0100 - 0.150 %Average value: 0.0388 % Grade Count:40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Carbon Steel
Overview of materials for AISI 4000 Series Steel
Overview of materials for Medium Alloy Steel
Overview of materials for High Carbon Steel
Overview of materials for Stainless Steel

M01005 / 81723

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.