MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ThyssenKrupp XABO® 460 T Structural Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-bar impact test.

Application: These steels are applied in welded constructions such as supporting structures, vessels etc., where a secured prevention against cold cracking in the welded joints is required. Due to the low carbon equivalent, these steels are highly resistant against cold cracking.

Information Provided by Thyssen Krupp

Key Words: S460ML; EN 1.8838
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 530 - 720 MPa76900 - 104000 psi
Tensile Strength, Yield >= 420 MPa>= 60900 psi50
 >= 440 MPa>= 63800 psi35
 >= 460 MPa
@Thickness 35.0 mm
>= 66700 psi
@Thickness 1.38 in
Elongation at Break >= 17 %>= 17 %
Modulus of Elasticity 213 GPa30900 ksi
Charpy Impact  16.0 J
@Temperature -50.0 °C
11.8 ft-lb
@Temperature -58.0 °F
Transverse
 25.0 J
@Temperature -40.0 °C
18.4 ft-lb
@Temperature -40.0 °F
Transverse
 27.0 J
@Temperature -50.0 °C
19.9 ft-lb
@Temperature -58.0 °F
Longitudinal
 35.0 J
@Temperature -30.0 °C
25.8 ft-lb
@Temperature -22.0 °F
Transverse
 40.0 J
@Temperature -40.0 °C
29.5 ft-lb
@Temperature -40.0 °F
Longitudinal
 45.0 J
@Temperature -20.0 °C
33.2 ft-lb
@Temperature -4.00 °F
Transverse
 50.0 J
@Temperature -30.0 °C
36.9 ft-lb
@Temperature -22.0 °F
Longitudinal
 65.0 J
@Temperature -20.0 °C
47.9 ft-lb
@Temperature -4.00 °F
Longitudinal
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.000030 ohm-cm0.000030 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.450 J/g-°C0.108 BTU/lb-°F
Thermal Conductivity 45.0 W/m-K312 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.14 %<= 0.14 %
Copper, Cu <= 0.30 %<= 0.30 %
Iron, Fe >= 96.4 %>= 96.4 %As Balance
Manganese, Mn <= 1.7 %<= 1.7 %
Nickel, Ni <= 0.40 %<= 0.40 %
Niobium, Nb (Columbium, Cb) <= 0.050 %<= 0.050 %
Other <= 0.45 %<= 0.45 %Carbon Equivalent
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.010 %<= 0.010 %
 
Descriptive Properties
Magnetic Propertiesmagnetizable
Thermal diffusivity (cm²/s)0.13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ThyssenKrupp XABO® 460 Structural Steel
ThyssenKrupp PAS 460 Structural Steel for Cold Forming
ASTM A131 Steel, Grade CS
Evonik TEGO® Flow ZFS 460
ThyssenKrupp XAR® 450 Structural Steel

NTHYSS012 / 90332

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.