MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Baystar™ 6410 HDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPE

Applications: paper overwrap, cup overwrap, plate overwrap, envelope windows, release liners, stand-up bags, specialty monolayer films, coextruded films

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture.

Key Words: Clarity Medium Molecular Weight
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.956 g/cc0.0345 lb/in³ASTM D-792
Water Vapor Transmission 1.55 g/m²/day0.100 g/100 in²/dayASTM F-1294
Melt Flow 1.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 900 %900 %ASTM D-882, A
Film Elongation at Break, TD 1100 %1100 %ASTM D-882, A
Elmendorf Tear Strength MD 38 g38 gASTM D1922
Elmendorf Tear Strength TD 100 g100 gASTM D1922
Film Tensile Strength at Break, MD 32.4 MPa4700 psiASTM D-882, A
Film Tensile Strength at Break, TD 32.4 MPa4700 psiASTM D-882, A
1% Secant Modulus, MD 689 MPa100000 psiASTM D-882, A
1% Secant Modulus, TD 903 MPa131000 psiASTM D-882, A
 
Thermal PropertiesMetricEnglishComments
Melting Point 134 °C273 °FASTM D-3417
 
Optical PropertiesMetricEnglishComments
Haze 24 %24 %ASTM D1003
Gloss 36 %36 %45°; ASTM D523
 
Descriptive Properties
processFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Equate EMDA-8920 HDPE Injection Molding Resin
Ipiranga Petrochem GF 5150 HDPE
Braskem Prisma® 6410 Extrusion Blow Molding Polypropylene
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene
Braskem HD3000N HDPE Cast Film Extrusion Polyethylene Homopolymer

PBAYST809 / 38677

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.