Product Description: UL 15028EM1 is a copolymer of ethylene and vinyl acetate. Availability: Africa & Middle East and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
- Free Flowing Agent: Yes
Applications:Information provided by ExxonMobil |