MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Elastosil® FLR 3900/40 A/B Liquid Fluorosilicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Fluorosilicone (FVMQ) of the ELASTOSIL® FLR 3900 series are paste-like, easily-pigmentable two component compounds. Its vulcanizates are noted for their excellent resistance against fuel and oil.

Application: Grades of ELASTOSIL® FLR 3900 can be used for sealants in aviation and automotive industry. Parts made from ELASTOSIL® FLR 3900 can generally be used for technical applications, but do not comply with regulations in the pharmaceutical and food industry.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ISO 1183-1 A
Viscosity 500000 cP
@Shear Rate 10.0 1/s
500000 cP
@Shear Rate 10.0 1/s
DIN 53019
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4444DIN 53505
Tensile Strength at Break 7.00 MPa1020 psiDIN 53504 S 1
Elongation at Break 400 %400 %DIN 53504 S 1
Tear Strength 20.0 kN/m114 pliASTM 624 B
Compression Set  14 %
@Temperature 150 °C,
Time 79200 sec
14 %
@Temperature 302 °F,
Time 22.0 hour
post cure 1h/100°C; DIN ISO 815-B
 18 %
@Temperature 150 °C,
Time 79200 sec
18 %
@Temperature 302 °F,
Time 22.0 hour
DIN ISO 815-B
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
0.0833 hour
@Treatment Temp. 329 °F
in press
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Rogers Arlon 31140R020 0.020" (0.508 mm) Uncured Fluorosilicone Rubber on Release Carrier
Wacker Elastosil® LR 3003/40 A/B Liquid Silicone Rubber
Freudenberg F40 Fluorosilicone Elastomer
Dow Silastic® LS 4-9038 FLUOROSILICONE RUBBER

PWACK9078 / 204607

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.