MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® GLT-600S Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Cures exceptionally fast to a high state of cure
  • Similar to improved low temperature properties compared to Viton® GLT
  • Improved mold release/mold fouling properties
  • Improved mold flow and less shear sensitivity for a 65 Mooney peroxy cured FKM
  • Excellent physical properties with high elongation, both original and aged
  • Heat, fluids, and low temperature resistance comparable to Viton® GLT
  • Improved water resistance / lower volume swell in water
  • Excellent compression set resistance with either low or no postcure

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/ccUncompounded Viton
Mooney Viscosity 65
@Temperature 121 °C
65
@Temperature 250 °F
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6565No Postcure; ASTM D1414
 67672 hours Postcure; ASTM D1414
Tensile Strength at Break 13.2 MPa1910 psiNo Postcure; ASTM D412
 17.8 MPa2580 psi2 hours Postcure; ASTM D412
Tensile Stress at Strain  0.600 MPa
@Strain 10 %
87.0 psi
@Strain 10 %
No Postcure; ASTM D412
 0.600 MPa
@Strain 10 %
87.0 psi
@Strain 10 %
2 hours Postcure; ASTM D412
Elongation at Break 267 %267 %2 hours Postcure; ASTM D412
 292 %292 %No Postcure; ASTM D412
100% Modulus  3.20 MPa
@Strain 100 %
464 psi
@Strain 100 %
No Postcure; ASTM D412
 3.60 MPa
@Strain 100 %
522 psi
@Strain 100 %
2 hours Postcure; ASTM D412
Compression Set  11 %
@Temperature 200 °C,
Time 79200 sec
11 %
@Temperature 392 °F,
Time 22.0 hour
O-Rings, postcured; ASTM D395B
 16 %
@Temperature 200 °C,
Time 79200 sec
16 %
@Temperature 392 °F,
Time 22.0 hour
O-Rings, no postcure; ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -31.4 °C-24.5 °FRetraction Temperature, Tr10
Glass Transition Temp, Tg -32.9 °C-27.2 °FPostcured
 
Processing PropertiesMetricEnglishComments
Processing Temperature  177 °C
@Time 421 sec
351 °F
@Time 0.117 hour
Cure
 232 °C
@Time 7200 sec
450 °F
@Time 2.00 hour
Postcure
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 64 %64 %Uncompounded Viton
 
Descriptive Properties
Colorwhite to tanUncompounded Viton
Compound NumberA22-03
FormsheetUncompounded Viton
Formulation as Tested100GLT-600S
 3Luperox® 101-XL45
 3Diak 7 (TAIC)
 3Zinc Oxide
 30MT Black
OdornoneUncompounded Viton
Storage StabilityExcellentUncompounded Viton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Freudenberg V115 Standard Fluoroelastomer
Freudenberg V123 Standard Fluoroelastomer
Chemours Viton® GFLT-600S with MgO/ZnO Fluoroelastomer Compound
Freudenberg V141 Standard Fluoroelastomer
Chemours Viton® B-70 Fluoroelastomer (FKM), Low Temperature Grade

PDVC9852 / 170493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.