MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Escorene® UL 7765 Adhesive Application Resin
Categories: Polymer; Adhesive; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Escorene Ultra UL 7765 is a high viscosity, 26.2% vinyl acetate copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt adhesives, sealants and wax blends. The resin accepts high filler level and is therfore suitable for W&C applications, in particular for haolgen free, flame retardant compounds.

Availability: Asia Pacific, Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Adhesives and Sealants
  • Hot Melt Adhesives
  • Industrial Sealants
  • Wax Blends
  • Bonding Adhesives
  • Wire and Cable Compounds
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³ExxonMobil Method
Vinyl Acetate Content 26.2 %26.2 %ExxonMobil Method
Melt Flow 2.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 828215s; ASTM D2240
Hardness, Shore D 232315s; ASTM D2240
Tensile Strength at Break 11.7 MPa1700 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus, 1% Secant 29.6 MPa4300 psiASTM D790
Dart Drop, Total Energy  21.7 J
@Temperature 22.8 °C
16.0 ft-lb
@Temperature 73.0 °F
ASTM D3736
 24.4 J
@Temperature -40.0 °C
18.0 ft-lb
@Temperature -40.0 °F
ASTM D3736
 
Thermal PropertiesMetricEnglishComments
Melting Point 73.9 °C165 °FPeak Melting Temperature; ExxonMobil Method
 
Descriptive Properties
FeaturesThermal Stabilizer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Escorene® MV 02514 EVA Copolymer, Adhesive and Sealant Grade
ExxonMobil EVA 14018.07 Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
Dow Elvaloy® 4924 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer
Dow Elvax® 3134SBZ Ethylene Vinyl Acetate
ExxonMobil Escorene® UL 7710 Adhesive Application Resin

PEXB164 / 37469

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.