MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Luranyl® KR 2454/3 G4 Polyphenylene Ether + Styrene-Butadiene Blend, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled; Styrene-Butadiene

Material Notes: Glass fiber reinforced grade containing halogen-free flame-retardant; for moldings with high heat resistance and stiffness (e.g. relay parts, controller and switch housings).

Data was collected by ISO methods and provided by BASF.

Key Words: PPE + SBS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³
Water Absorption 0.40 %0.40 %
Moisture Absorption at Equilibrium 0.15 %0.15 %
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/in
High Load Melt Index 15 g/10 min
@Load 21.6 kg,
Temperature 250 °C
15 g/10 min
@Load 47.6 lb,
Temperature 482 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 90.0 MPa13100 psi
Elongation at Break 3.0 %3.0 %
Tensile Modulus 6.50 GPa943 ksi
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
Dielectric Strength 85.0 kV/mm2160 kV/in
Dissipation Factor 0.0030
@Frequency 1e+6 Hz
0.0030
@Frequency 1e+6 Hz
Comparative Tracking Index 225 V225 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
@Temperature 20.0 °C
19.4 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 140 °C284 °F
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °F
Vicat Softening Point 142 °C288 °F
Flammability, UL94 V-1
@Thickness 3.20 mm
V-1
@Thickness 0.126 in
Oxygen Index 29 %29 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Luranyl® KR 2454/3 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced
BASF Luranyl® KR 2452/3 Polyphenylene Ether + Styrene-Butadiene Blend
BASF Luranyl® KR 2451/3 Polyphenylene Ether + Styrene-Butadiene Blend
BASF Luranyl® KR 2450/3 Polyphenylene Ether + Styrene-Butadiene Blend
BASF Luranyl® KR 2420 Polyphenylene Ether + Styrene-Butadiene Blend

PSF116 / 66697

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.