MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay AVIMID® RB Polyimide Composite
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: Description: AVIMID® RB is a high temperature, 644°F (340°C) Tg* thermoset polyimide resin with wet service capability to more than 530°F (277°C) and dry service capability of 600°F (316°C). AVIMID RB has excellent thermal oxidative stability and resistance to aircraft fluids. AVIMID RB was formulated for prepreg autoclave vacuum bag processing, but can be successfully compression molded both as a prepreg and in dry forms as neat resin or chopped-fiber molding compound. Unidirectional tape and woven prepreg of AVIMID RB will retain their tack and drape for 14 days at 70°F (21°C). Standard autoclave or compression molding processes, to a final temperature of 680°F (360°C) will result in full Tg development/cure with no need for post-cure treatment. AVIMID RB can be solution impregnated on a variety of fibers and fabrics.

Features & Benefits:

  • High Tg, 644°F (340°C)*
  • Non-MDA, PMR-15 replacement; no carcinogenic components
  • Service temperature >530°F (277°C) wet and 600°F (316°C) dry
  • Specified for jet engine use
  • Autoclave and press mold processing
  • Available in a range of fibers and forms including tape, fabric, chopped fiber and neat resin
  • No post-cure needed
  • 680°F (360°C) final cure
  • Shelf life of 12 months at 0°F (-18°C), 14 days at 70°F (21°C)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 2.00e+8 cP
@Temperature 316 °C
2.00e+8 cP
@Temperature 601 °F
Melt
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 82.7 MPa12000 psi
 745 MPa108000 psi0°, T650-35 carbon fiber reinforced 8 harness satin fabric
Elongation at Break 2.4 %2.4 %
Tensile Modulus 3.80 GPa551 ksi
 71.5 GPa10400 ksi0°, T650-35 carbon fiber reinforced 8 harness satin fabric
Flexural Strength 111 MPa16100 psi
Flexural Modulus 3.80 GPa551 ksi
Compressive Strength  449 MPa
@Temperature 288 °C
65100 psi
@Temperature 550 °F
0°, T650-35 carbon fiber reinforced 8 harness satin fabric
 481 MPa
@Temperature 232 °C
69800 psi
@Temperature 450 °F
0°, T650-35 carbon fiber reinforced 8 harness satin fabric
 796 MPa
@Temperature 22.0 °C
115000 psi
@Temperature 71.6 °F
0°, T650-35 carbon fiber reinforced 8 harness satin fabric
Shear Modulus 5.10 GPa740 ksiIn-plane
Shear Strength 84.1 MPa12200 psiIn-plane
 55.2 MPa
@Temperature 316 °C
8000 psi
@Temperature 601 °F
0°, Interlaminar, T650-35 carbon fiber reinforced 8 harness satin fabric
 57.9 MPa
@Temperature 232 °C
8400 psi
@Temperature 450 °F
0°, Interlaminar, T650-35 carbon fiber reinforced 8 harness satin fabric
 68.9 MPa
@Temperature 22.0 °C
10000 psi
@Temperature 71.6 °F
0°, Interlaminar, T650-35 carbon fiber reinforced 8 harness satin fabric
 72.4 MPa
@Temperature 177 °C
10500 psi
@Temperature 351 °F
0°, Interlaminar, T650-35 carbon fiber reinforced 8 harness satin fabric
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 277 °C531 °Fwet
 316 °C601 °Fdry
Glass Transition Temp, Tg 277 °C531 °FWet
 340 °C644 °FDry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay AVIMID® N Polyimide Composite
Mitsubishi Chemical Advanced Materials Semitron™ ESd 480 PEEK, static dissipative
Röchling Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod
Solvay AVIMID® R Polyimide Composite
Arlon Electronic Materials 84N Polyimide Laminate and Prepreg

PCYTED077 / 180379

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.