MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Melinex® 331 Polyester Film, 200 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.

Approvals: UL Recognition - Product has been registered with Underwriters Laboratories

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ASTM D1505
Thickness 50.8 microns2.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 86.2 MPa12500 psiASTM D882A
Film Tensile Strength at Yield, TD 86.2 MPa12500 psiASTM D882A
Film Elongation at Break, MD 135 %135 %ASTM D882A
Film Elongation at Break, TD 95 %95 %ASTM D882A
Coefficient of Friction, Dynamic 0.30 - 0.400.30 - 0.40A-B; ASTM D1894
Coefficient of Friction, Static 0.30 - 0.400.30 - 0.40ASTM D1894
Film Tensile Strength at Break, MD 159 MPa23000 psiASTM D882A
Film Tensile Strength at Break, TD 186 MPa27000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 2.8 %
@Temperature 190 °C,
Time 300 sec
2.8 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 190 °C,
Time 300 sec
1.0 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Gloss 40 %40 %45°; ASTM D1003
 45 %45 %60°; ASTM D1003
Transmission, Visible 12 %12 %TLT; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 339 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 329 Polyester Film, 1400 Gauge
DuPont Teijin Films Melinex® 329 Polyester Film, 1000 Gauge
DuPont Teijin Films Melinex® 331 Polyester Film, 700 Gauge
DuPont Teijin Films Melinex® 331 Polyester Film, 300 Gauge

PDTZ9045 / 139442

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.