MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott Glass 8360 Lead-Free Soft Glass
Categories: Ceramic; Glass

Material Notes: Soft glass, lead-free

Encapsulation of semiconductor components at low temperature (diodes)

The heavy metal content for the elements lead, mercury, cadmium, and hexavalent chromium is less than 100 ppm

Information provided by SCHOTT AG.

Vendors: SCHOTT with its Business Unit Tubing offers tailor-made products & services worldwide from more than sixty special glass types for international growth markets such as industrial and environmental technology, electronics, display industry, architecture and design as well as pharmaceuticals. Contact us.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc
@Temperature 25.0 °C
0.0961 lb/in³
@Temperature 77.0 °F
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 44DIN 12116
Alkali Class, AR 33ISO 695
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 85.0 GPa12300 ksi
Poissons Ratio 0.240.24
Shear Modulus 34.3 GPa4970 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  5.00e+6 ohm-cm
@Temperature 350 °C
5.00e+6 ohm-cm
@Temperature 662 °F
 3.20e+8 ohm-cm
@Temperature 250 °C
3.20e+8 ohm-cm
@Temperature 482 °F
Dielectric Constant 7.3
@Frequency 1e+6 Hz,
Temperature 25.0 °C
7.3
@Frequency 1e+6 Hz,
Temperature 77.0 °F
Dielectric Loss Index 0.0024
@Frequency 1e+6 Hz,
Temperature 25.0 °C
0.0024
@Frequency 1e+6 Hz,
Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.10 µm/m-°C
@Temperature 20.0 - 300 °C
5.06 µin/in-°F
@Temperature 68.0 - 572 °F
ISO 7991
Transformation Temperature, Tg 465 °C869 °FISO 7884-8
Softening Point 575 °C1070 °FViscosity 107.6 dPa s; ISO 7884-3
Working Point 745 °C1370 °FViscosity 104 dPa s; ISO 7884-2
Annealing Point 470 °C878 °FViscosity 1013 dPa s; ISO 7884-4
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.566
@Wavelength 587.6 nm
1.566
@Wavelength 587.6 nm
 
Descriptive Properties
Hydrolytic ResistanceClass HGB 3ISO 719
Stress-optical Coefficient K (10-6mm2N-1)2.9DIN 52314
tk100(°C)275

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott Glass 8531 Soft Glass
Schott Glass 8532 Soft Glass
Schott Glass 8436
Schott G018-117 Dental Glass
Schott G018-093 Dental Glass

CSGS925 / 162030

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.