MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Dow 3110 SILICONE RUBBER ENCAPSULANT
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc
@Temperature 25.0 °C
1.14 g/cc
@Temperature 77.0 °F
Viscosity 13000 cP13000 cPdynamic
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545
Tensile Strength, Ultimate 2.76 MPa400 psi
Elongation at Break 175 %175 %
Tear Strength 3.51 kN/m20.0 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.30e+12 ohm-cm7.30e+12 ohm-cm
Dielectric Constant  2.2
@Frequency 100000 Hz
2.2
@Frequency 100000 Hz
 2.29
@Frequency 100 Hz
2.29
@Frequency 100 Hz
Dielectric Strength 17.1 kV/mm434 kV/in
Dissipation Factor  0.0010
@Frequency 100000 Hz
0.0010
@Frequency 100000 Hz
 0.010
@Frequency 100 Hz
0.010
@Frequency 100 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
Colorwhite
Mix Ratio (X:1)10Base to Catalyst ETN

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 25150-G SILICONE RUBBER
Dow 3112 RTV SILICONE RUBBER
Multibase C6-515 Dow-Corning Class VI Elastomer
Dow Silastic® 1604-T SILICONE RUBBER
Dow 3120 RTV SILICONE RUBBER

PDOWCO379 / 106080

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.