MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled; Polyethylene Terephthalate (PET)

Material Notes: Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housings for vehicles, headlamp frames, cams, automotive windscreen wiper arms, PCBs, housings, consoles, contact mounts and covers.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %0.40 %DIN 53495/1L
Viscosity Test 107 cm³/g1.07 dl/gViscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inSheet
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inSheet
Melt Flow 33.36 g/10 min
@Load 2.16 kg,
Temperature 275 °C
33.36 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 96.0 MPa13900 psi50 mm/min; ISO 527-2
Elongation at Yield 2.9 %2.9 %50 mm/min; ISO 527-2
Modulus of Elasticity 5.00 GPa725 ksiISO 527-2
Charpy Impact Unnotched 2.60 J/cm²12.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.380 J/cm²1.81 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 - 250 °C428 - 482 °FDSC; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 216 °C421 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 168 °C334 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °FInjection-molding
 270 °C518 °Ffor shrinkage test
Mold Temperature 60.0 - 100 °C140 - 212 °F
 80.0 °C176 °Ffor shrinkage test
 
Descriptive Properties
ColorColored and Black
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET
BASF Petra® 7010 WT 7729 15% Glass Filled PET
BASF Petra® 7010 BK 5830 15% Glass Filled PET

PBASG0094 / 131728

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.