MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1701 FR Modified Polyphenylene Oxide (PPO), Glass Fiber - Flame Retardant - Halogen Free
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 10% Glass Filled

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D 792
Filler Content 10 %10 %Primary Additive
Water Absorption 0.080 %0.080 %24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
@Thickness 3.17 mm
0.0030 - 0.0050 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.8 MPa11000 psiASTM D 638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %ASTM D 638
Tensile Modulus 4.48 GPa650 ksiASTM D 638
Flexural Strength 103 MPa15000 psiASTM D 790
Flexural Modulus 4.14 GPa600 ksiASTM D 790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.17 mm
10.0 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 249 - 288 °C480 - 550 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 93.3 °C200 °F
Dry Time 2 hour2 hour
Moisture Content 0.10 %0.10 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 1700 FR Modified Polyphenylene Oxide (PPO), Flame Retardant - Halogen Free
RTP Company RTP 1701 Modified Polyphenylene Oxide (PPO), Glass Fiber
RTP Company RTP 1799 x 117570 A Modified Polyphenylene Oxide (PPO), Electrically Conductive - Flame Retardant
RTP Company EMI 1761  Modified Polyphenylene Oxide (PPO) Shielding - Stainless Steel Fiber 10%
RTP Company ESD 1783 Modified Polyphenylene Oxide (PPO); Carbon Fiber - Electrically Conductive - EMI/RFI Shielding

PQZWA2304 / 91088

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.