MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxy Technology EPO-TEK® T7109 Thermally Conductive Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Product Description: EPO-TEK® T7109 is a two component, thermally conductive epoxy designed for die attach and heat-sinking applications found in the semiconductor, hybrid, medical and optical industries.

Advantages & Application Notes:

  • Reliability report available describing its performance
    • Thermal resistance compared to three other epoxies
    • Thermal resistance and how it relates to overall thermal conductivity
    • Strength measurements plotted versus pot-life, versus Tcycles and damp heat (85°C/85%RH).
  • Thixotropic paste allows for application by automatic dispensers or screen printers. It can also be applied by hand or spatula.
  • Excellent adhesion to Aluminum, ferrous and non ferrous metals, and most plastics including Kapton.
  • Suggested Applications:
    • Semiconductor - Thermally conductive underfill / Electrically non conductive die-attach, low stress for large die exceeding 500 mil x 500 mil.
    • Hybrid Micro-electronics - Large die attach, adhesion to GaAs devices, ceramic substrate attach to housing
    • Fiber Optic Packaging - Substrate attach of optical bench; TECooler attach; good adhesion to Au, Kovar and ceramic; can be used for laser diode and photo-diode attach.
    • Liquid Crystal Displays - die-attach micro-LCDs onto flex circuits like Kapton, or rigid carriers like FR4, ceramic, or silicon.
    • Medical - Heat sinking electronics found in ultrasound and CT Detectors, and other radiation devices.
  • Low temperature cure between 80°C and 150°C allows use on lower cost plastics and temperature sensitive devices.
  • Can be suggested as a lower stress, more resilient alternative of EPO-TEK® 930-4.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccPart B
 1.33 g/cc1.33 g/ccPart A
Particle Size <= 20 µm<= 20 µm
Viscosity 14000 - 20000 cP
@Temperature 23.0 °C
14000 - 20000 cP
@Temperature 73.4 °F
20 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383
Tensile Modulus 1.78 GPa258 ksiStorage
Shear Strength >= 13.8 MPa>= 2000 psiLap
 >= 35.2 MPa>= 5100 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 8.00e+12 ohm-cm>= 8.00e+12 ohm-cm
Dielectric Constant 3.5
@Frequency 1000 Hz
3.5
@Frequency 1000 Hz
Dissipation Factor 0.0040
@Frequency 1000 Hz
0.0040
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.0 µm/m-°C25.6 µin/in-°FBelow Tg
 239 µm/m-°C133 µin/in-°FAbove Tg
Thermal Conductivity  0.700 W/m-K
@Thickness 1.02 mm
4.86 BTU-in/hr-ft²-°F
@Thickness 0.0402 in
 1.50 W/m-K
@Thickness 0.0762 mm
10.4 BTU-in/hr-ft²-°F
@Thickness 0.00300 in
Maximum Service Temperature, Air 200 °C392 °FContinuous
 300 °C572 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 45.0 °C>= 113 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 377 °C711 °FDegradation Temperature
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 150 °C
0.167 hour
@Temperature 302 °F
Minimum Bond Line
 480 min
@Temperature 80.0 °C
8.00 hour
@Temperature 176 °F
Minimum Bond Line
Pot Life 240 min240 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorAmberPart B
 WhitePart A
ConsistencySmooth paste
Number of ComponentsTwo
Weight Loss0.02%200°C
 0.25%250°C
 0.98%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil EPM-2890 Silicone, Thermal Interface Material (TIM): Adhesive
Raschig Group MELOPLAS® 181.5 MF
Tropical Iroko Wood
Epoxy Technology EPO-TEK® 920 Thermally Conductive Epoxy
Abatron WoodEpox® Wood Replacement Compound

PPOXYT092 / 141131

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.