MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Palladium Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Palladium Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Palladium Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.08 - 15.8 g/cc0.256 - 0.571 lb/in³Average value: 11.6 g/cc Grade Count:56
Particle Size 0.150 µm0.150 µmAverage value: 0.150 µm Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 78.0 - 27778.0 - 277Average value: 130 Grade Count:14
Hardness, Knoop 109 - 331109 - 331Average value: 161 Grade Count:12
Hardness, Rockwell A 48.0 - 66.048.0 - 66.0Average value: 52.7 Grade Count:6
Hardness, Rockwell B 29.0 - 86.029.0 - 86.0Average value: 63.6 Grade Count:12
Hardness, Rockwell 15T 57.0 - 93.057.0 - 93.0Average value: 82.3 Grade Count:10
Hardness, Vickers 37.0 - 45037.0 - 450Average value: 182 Grade Count:30
Tensile Strength, Ultimate 172 - 1330 MPa24900 - 193000 psiAverage value: 483 MPa Grade Count:36
Tensile Strength, Yield 260 - 990 MPa37700 - 144000 psiAverage value: 581 MPa Grade Count:11
Elongation at Break 2.00 - 47.0 %2.00 - 47.0 %Average value: 16.0 % Grade Count:32
Modulus of Elasticity 96.0 - 141 GPa13900 - 20500 ksiAverage value: 118 GPa Grade Count:18
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000993 - 0.0000430 ohm-cm0.00000993 - 0.0000430 ohm-cmAverage value: 0.0000262 ohm-cm Grade Count:37
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.1 - 16.8 µm/m-°C6.17 - 9.33 µin/in-°FAverage value: 13.6 µm/m-°C Grade Count:25
Specific Heat Capacity 0.195 - 0.247 J/g-°C0.0466 - 0.0590 BTU/lb-°FAverage value: 0.239 J/g-°C Grade Count:7
Thermal Conductivity 37.2 - 76.0 W/m-K258 - 527 BTU-in/hr-ft²-°FAverage value: 67.7 W/m-K Grade Count:10
Melting Point 820 - 1650 °C1510 - 3000 °FAverage value: 1320 °C Grade Count:32
Solidus 820 - 1560 °C1510 - 2840 °FAverage value: 1170 °C Grade Count:20
Liquidus 960 - 1650 °C1760 - 3000 °FAverage value: 1250 °C Grade Count:20
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.3300.330Average value: 0.330 Grade Count:7
Reflection Coefficient, Visible (0-1) 0.628 - 0.6300.628 - 0.630Average value: 0.630 Grade Count:7
 
Processing PropertiesMetricEnglishComments
Processing Temperature 699 - 1230 °C1290 - 2250 °FAverage value: 895 °C Grade Count:13
Casting Temperature 1210 - 1420 °C2210 - 2590 °FAverage value: 1360 °C Grade Count:10
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 4.00 - 40.0 %4.00 - 40.0 %Average value: 17.5 % Grade Count:9
Gallium, Ga 1.50 - 9.00 %1.50 - 9.00 %Average value: 5.00 % Grade Count:5
Gold, Au 2.00 - 57.5 %2.00 - 57.5 %Average value: 23.9 % Grade Count:11
Indium, In 0.900 - 9.00 %0.900 - 9.00 %Average value: 4.98 % Grade Count:5
Nickel, Ni 1.00 - 75.6 %1.00 - 75.6 %Average value: 25.0 % Grade Count:10
Palladium, Pd 23.0 - 100 %23.0 - 100 %Average value: 70.1 % Grade Count:57
Platinum, Pt 1.00 - 40.0 %1.00 - 40.0 %Average value: 14.8 % Grade Count:8
Ruthenium, Ru 0.100 - 11.0 %0.100 - 11.0 %Average value: 3.92 % Grade Count:12
Silver, Ag 2.00 - 63.5 %2.00 - 63.5 %Average value: 30.8 % Grade Count:27
Tin, Sn 2.70 - 9.00 %2.70 - 9.00 %Average value: 4.80 % Grade Count:4
Zinc, Zn 1.00 - 2.50 %1.00 - 2.50 %Average value: 1.83 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Copper Alloy
Overview of materials for Silver Alloy
Overview of materials for Refractory Metal
Overview of materials for Gold Alloy
Overview of materials for Molybdenum Alloy

M01064 / 81695

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.