MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BCC Products BC 4578 Polyester Model Board Filler
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: BC 4578 is a quick setting easy to use filler paste which is designed specifically for repair to Model Board MB 2001. Its lightweight characteristic and tack free cure makes for ease of finishing with simple woodworking tools. Area to be filled should be clean and dry, free from dust, oil and release agents. It is advisable to scarify the area prior to application. May be applied at any reasonable thickness by spreading or splining. Do not work with more material than can be applied in 5 minutes. Material mixed with cream hardener should not be returned to original can. After final cure, material may be scraped, sanded, filed, drilled, tapped or machined to a feather edge.

Information provided by BCC Products, Inc.

Key Words: MB 2001
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 75.0 min
@Temperature 24.0 °C
0.750 - 1.25 hour
@Temperature 75.2 °F
Pot Life 5.0 - 10 min
@Temperature 24.0 °C
5.0 - 10 min
@Temperature 75.2 °F
1 lb mass
Shelf Life 6.00 Month6.00 Monthin tightly closed container
 
Descriptive Properties
Mix Ratio100:1 or 100:2 resin/hardener
Mixed Viscosity, BrookfieldThixotropic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cosmic Plastics D62 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade
Plenco 4300 Phenolic, Granular, Transfer Molded
Plenco 4300 Phenolic, Granular, Injection Molded
Plenco 4300 Phenolic, Granular, Compression Molded

PBCC005 / 107232

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.