MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Heat Resistant Grade, Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 - 1.61 g/cc0.0531 - 0.0582 lb/in³Average value: 1.52 g/cc Grade Count:12
Water Absorption 0.200 - 0.300 %0.200 - 0.300 %Average value: 0.240 % Grade Count:12
Linear Mold Shrinkage 0.00330 - 0.0120 cm/cm0.00330 - 0.0120 in/inAverage value: 0.00687 cm/cm Grade Count:12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 79.0 - 87.079.0 - 87.0Average value: 82.0 Grade Count:4
Tensile Strength, Ultimate 41.0 - 60.5 MPa5950 - 8770 psiAverage value: 50.5 MPa Grade Count:12
Elongation at Break 0.740 - 0.860 %0.740 - 0.860 %Average value: 0.813 % Grade Count:4
Modulus of Elasticity 8.80 - 13.1 GPa1280 - 1900 ksiAverage value: 10.3 GPa Grade Count:6
Flexural Yield Strength 69.0 - 89.8 MPa10000 - 13000 psiAverage value: 78.9 MPa Grade Count:12
Flexural Modulus 8.16 - 10.4 GPa1180 - 1510 ksiAverage value: 9.12 GPa Grade Count:10
Compressive Yield Strength 145 - 221 MPa21000 - 32100 psiAverage value: 195 MPa Grade Count:12
Charpy Impact, Notched 0.170 - 0.210 J/cm²0.809 - 0.999 ft-lb/in²Average value: 0.188 J/cm² Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.35e+11 - 2.68e+12 ohm-cm1.35e+11 - 2.68e+12 ohm-cmAverage value: 9.78e+11 ohm-cm Grade Count:12
Dielectric Constant 4.80 - 14.04.80 - 14.0Average value: 6.62 Grade Count:12
Dielectric Strength 7.40 - 16.7 kV/mm188 - 424 kV/inAverage value: 12.6 kV/mm Grade Count:12
Dissipation Factor 0.0370 - 0.1700.0370 - 0.170Average value: 0.0726 Grade Count:12
Arc Resistance 150 - 180 sec150 - 180 secAverage value: 165 sec Grade Count:6
Comparative Tracking Index 175 - 230 V175 - 230 VAverage value: 193 V Grade Count:12
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 - 205 °C302 - 401 °FAverage value: 186 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 166 - 204 °C331 - 399 °FAverage value: 180 °C Grade Count:12
UL RTI, Electrical 150 °C302 °FAverage value: 150 °C Grade Count:6
UL RTI, Mechanical with Impact 150 °C302 °FAverage value: 150 °C Grade Count:6
UL RTI, Mechanical without Impact 150 °C302 °FAverage value: 150 °C Grade Count:6
Flammability, UL94 V-1 - 5VAV-1 - 5VAGrade Count:12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic; Unreinforced; Molded
Overview of materials for Thermoset Polyester Glass Filled BMC
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
Overview of materials for Melamine-Phenolic Copolymer
Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System

O2701 / 78084

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.