MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMELT® A6560 Polyamide  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product properties: Evonik’s VESTAMELT®iS combines good adhesion to various substrates, good chemical resistance and excellent mechanical properties with high transparency. This offers prospects for new product designs that have been unavailable to date, particularly in the area of LED lighting and sensor products where transparency is a must.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Viscosity 38 cP
@Temperature 200 °C
38 cP
@Temperature 392 °F
Melt
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060JIS K7215
Tensile Strength at Break 40.0 MPa5800 psi
Elongation at Break 400 %400 %
Tensile Modulus 0.230 GPa33.4 ksi
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched NBNBISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmJIS K6911
Dielectric Constant 3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
VDE 303
Dielectric Strength 23.0 kV/mm584 kV/inIEC 60243-1
Dissipation Factor 0.058
@Frequency 1e+6 Hz
0.058
@Frequency 1e+6 Hz
VDE 303
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
Melting Point 165 °C329 °FISO 1346
Maximum Service Temperature, Air 100 °C212 °F
Vicat Softening Point 117 °C243 °FISO 306
Minimum Service Temperature, Air -30.0 °C-22.0 °F
Glass Transition Temp, Tg -8.00 °C17.6 °F
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.521.52JIS K7215
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 220 °C374 - 428 °F
Nozzle Temperature 200 - 230 °C392 - 446 °F
Zone 1 130 - 140 °C266 - 284 °F
Zone 2 150 - 160 °C302 - 320 °F
Zone 3 180 - 200 °C356 - 392 °F
Mold Temperature >= 20.0 °C>= 68.0 °F
Drying Temperature 70.0 °C158 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
Colortransparent
Funnel20-30°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® TP-1020 PC, Unreinforced Transparent
Mitsubishi Xantar® SF 22 Polycarbonate
Evonik VESTAMELT® A6453 Polyamide
Arkema Kynar Superflex® 2500-20 PVDF
Arkema Kynar Flex® 3312 C PVDF

PEVONIL234 / 196438

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.