MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Kennametal Stellite Deloro® 40G
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Nickel base. Good combination of wear resistance, corrosion resistance, machinability, and repairability. Machined with tungsten carbide tools, using slow speeds and light feeds. Finish grinding achieved with vitrified silicon carbine wheels. Applications include bottle making mold components such as neck rings, half bushings, and die inserts, also used for sealing faces in values in both the oil and nuclear industries. Normally resistant to atmospheric, steams salt water and salt spray corrosion. Excellent oxidation resistance up to melting range. Satisfactory performance in many organic acids but high corrosion rates observed in hot, strong inorganic acids. Highly resistant to semi-molten glass. Normally used in the as-cast condition. Data provided by the manufacturer, Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.20 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 312312Converted from Rockwell C hardness.
Hardness, Knoop 372372Converted from Rockwell C hardness.
Hardness, Rockwell A 6767Converted from Rockwell C hardness.
Hardness, Rockwell B 107107Converted from Rockwell C hardness. Beyond normal Rockwell B range, for comparison only.
Hardness, Rockwell C 30 - 3830 - 38
Hardness, Vickers 326326Converted from Rockwell C hardness.
Tensile Strength, Ultimate 385 MPa55800 psi
Tensile Strength, Yield 350 MPa50800 psi
Elongation at Break 1.0 %1.0 %
Modulus of Elasticity 198 GPa28700 ksi
Charpy Impact, Unnotched 4.00 J
@Temperature 23.0 °C
2.95 ft-lb
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.4 µm/m-°C
@Temperature 20.0 - 100 °C
6.33 µin/in-°F
@Temperature 68.0 - 212 °F
 12.8 µm/m-°C
@Temperature 20.0 - 300 °C
7.11 µin/in-°F
@Temperature 68.0 - 572 °F
 13.4 µm/m-°C
@Temperature 20.0 - 500 °C
7.44 µin/in-°F
@Temperature 68.0 - 932 °F
 14.3 µm/m-°C
@Temperature 20.0 - 700 °C
7.94 µin/in-°F
@Temperature 68.0 - 1290 °F
 15.4 µm/m-°C
@Temperature 20.0 - 900 °C
8.56 µin/in-°F
@Temperature 68.0 - 1650 °F
Melting Point 985 - 1180 °C1810 - 2160 °F
Solidus 985 °C1810 °F
Liquidus 1180 °C2160 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 1.2 %1.2 %
Carbon, C 0.25 %0.25 %
Chromium, Cr 7.4 %7.4 %
Iron, Fe 5.3 %5.3 %
Nickel, Ni 82 %82 %As Remainder
Silicon, Si 4.0 %4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Deloro® 208 PM after P/M Processing
Kennametal Stellite Deloro® 208 PM cast
Kennametal Stellite Deloro® 711 PM cast
Kennametal Stellite Deloro® 716 PM cast
Kennametal Stellite Deloro® N-6 PM with P/M Processing

NDA40G / 16095

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.