MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Diamond, Polycrystalline
Categories: Carbon; Diamond

Key Words: Diamonds, Carbon, C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.00 - 4.00 g/cc0.108 - 0.145 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 49 - 7849 - 78GPa Microhardness
Vickers Microhardness 25 - 9825 - 98GPa Microhardness
Modulus of Elasticity 749 - 953 GPa109000 - 138000 ksi
Compressive Strength 1900 - 6900 MPa276000 - 1.00e+6 psivalues depend on grain size and Co content
Poissons Ratio 0.070 - 0.200.070 - 0.20
Fracture Toughness 6.00 - 8.80 MPa-m½5.46 - 8.01 ksi-in½values depend on grain size and Co content
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.50 - 3.80 µm/m-°C
@Temperature 25.0 - 100 °C
0.833 - 2.11 µin/in-°F
@Temperature 77.0 - 212 °F
Thermal Conductivity 1200 W/m-K8330 BTU-in/hr-ft²-°FThick film diamond made by SP3
 1800 W/m-K12500 BTU-in/hr-ft²-°FDe Beers thermal thick film synthetic diamond.
 
Descriptive Properties
ColorClearImpurities (i.e. Nitrogen) and irradiation can change color to yellow, green, blue, pink, or brown.
Crystal StructureCubicDiamond - Space Group Fd3m

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Diamond, Natural
Diamond, Synthetic
Diamond, thin film
BACT DLC Diamond-Like Coating
304 Stainless Steel (UNS S30400); Cold Finished and Annealed Bar

CDiamC / 773

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.