MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, closures and various food containers.

Regulatory Status: H6017 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.

Specific recommendations for processing H6017 can only be made when the processing conditions, equipment and end use application are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.593 - 0.625 g/cc0.0214 - 0.0226 lb/in³ASTM D1895
Density 0.960 g/cc0.0347 lb/in³ASTM D1505
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 190 °C
18 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 28.2 cm11.1 inEquistar test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272ASTM D2240
Tensile Strength at Break 29.6 MPa4300 psi50 mm/min; ASTM D638
Elongation at Break 12 %12 %50 mm/min; ASTM D638
Tensile Modulus 0.8680 GPa125.9 ksi1% Secant; 50mm/min; ASTM D638
 1.001 GPa145.2 ksi50mm/min; ASTM D638
Flexural Modulus 1.474 GPa213.8 ksi12.5 mm/min; ASTM D790
 1.118 GPa
@Strain 2 %
162.2 ksi
@Strain 2 %
Secant; 12.5 mm/min; ASTM D790
Flexural Modulus, 1% Secant 1369 MPa198500 psi2.5 mm/min; ASTM D790
Izod Impact, Notched 0.395 J/cm0.740 ft-lb/inASTM D256
 5.34 J/cm
@Temperature -18.0 °C
10.0 ft-lb/in
@Temperature -0.400 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Melting Point 133.0 °C271.4 °FASTM D3418
Crystallization Temperature 115.7 °C240.3 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C165 °FASTM D648
Vicat Softening Point 128 °C262 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 °C450 °F
Middle Barrel Temperature 243 °C470 °F
Front Barrel Temperature 246 °C475 °F
Nozzle Temperature 246 °C475 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Alathon® H5234 High Density Polyethylene
SCG Chemicals EL-Lene™ H5818J High Density Polyethylene Injection Molding
Dow DOWLEX™ IP-40 High Density Polyethylene
LyondellBasell Lupolen 6031 M HDPE, Injection Molding Grade
Bamberger Polymers Bapolene® 2035 High Density Polyethylene, Blow Molding Grade

PEQU0798 / 104154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.