MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials Vespel® SP-1 ISO Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Parts and stock shapes from unfilled PI (polyimide) resin for high purity and high temperature environments

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccASTM D 792
Water Absorption 0.24 %0.24 %Immersion 24h; ASTM D 570
 0.72 %
@Temperature 50.0 °C
0.72 %
@Temperature 122 °F
Immersion 48h; ASTM D 570
Moisture Absorption at Equilibrium 1.0 - 1.3 %1.0 - 1.3 %50% RH; ASTM D 570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 45 - 6045 - 60ASTM D 785
Tensile Strength, Ultimate  41.0 MPa
@Temperature 260 °C
5950 psi
@Temperature 500 °F
ASTM D 638
 86.0 MPa
@Temperature 23.0 °C
12500 psi
@Temperature 73.4 °F
ASTM D 638
Elongation at Break  6.0 %
@Temperature 260 °C
6.0 %
@Temperature 500 °F
ASTM D 638
 7.5 %
@Temperature 23.0 °C
7.5 %
@Temperature 73.4 °F
ASTM D 638
Flexural Strength  62.0 MPa
@Temperature 260 °C
8990 psi
@Temperature 500 °F
ASTM D 790
 110 MPa
@Temperature 23.0 °C
16000 psi
@Temperature 73.4 °F
ASTM D 790
Flexural Modulus  1.723 GPa
@Temperature 260 °C
249.9 ksi
@Temperature 500 °F
ASTM D 790
 3.101 GPa
@Temperature 23.0 °C
449.8 ksi
@Temperature 73.4 °F
ASTM D 790
Shear Strength 90.0 MPa13100 psiASTM D 732
Izod Impact, Notched 0.427 J/cm
@Temperature 23.0 °C
0.800 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 7.470 J/cm
@Temperature 23.0 °C
13.99 ft-lb/in
@Temperature 73.4 °F
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.00e+16 ohm-cm8.00e+16 ohm-cmASTM D 257
Surface Resistance 4.00e+12 ohm4.00e+12 ohmASTM D 257
Dielectric Constant  3.66
@Frequency 1e+6 Hz,
Temperature 23.0 °C
3.66
@Frequency 1e+6 Hz,
Temperature 73.4 °F
ASTM D 150
 3.73
@Frequency 10000 Hz,
Temperature 23.0 °C
3.73
@Frequency 10000 Hz,
Temperature 73.4 °F
ASTM D 150
 3.74
@Frequency 100 Hz,
Temperature 23.0 °C
3.74
@Frequency 100 Hz,
Temperature 73.4 °F
ASTM D 150
Dielectric Strength 24.6 kV/mm
@Thickness 2.00 mm,
Temperature 23.0 °C
625 kV/in
@Thickness 0.0787 in,
Temperature 73.4 °F
Short time; ASTM D149
Dissipation Factor  0.0015
@Frequency 100 Hz
0.0015
@Frequency 100 Hz
ASTM D 150
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
ASTM D 150
 0.0054
@Frequency 10000 Hz
0.0054
@Frequency 10000 Hz
ASTM D 150
Comparative Tracking Index 175 - 249 V175 - 249 VIEC 60112
 175 - 249 V
@Thickness 3.00 mm
175 - 249 V
@Thickness 0.118 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 360 °C680 °FASTM D 648
UL RTI, Electrical  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746B
 130 °C
@Thickness 1.70 mm
266 °F
@Thickness 0.0669 in
UL 746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical with Impact  130 °C
@Thickness 1.70 mm
266 °F
@Thickness 0.0669 in
UL 746B
 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746B
UL RTI, Mechanical without Impact  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746B
 130 °C
@Thickness 1.70 mm
266 °F
@Thickness 0.0669 in
UL 746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746B
Flammability, UL94  V-0
@Thickness 1.70 mm
V-0
@Thickness 0.0669 in
IEC 60695-11-10
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
IEC 60695-11-10
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
UL94
 V-0
@Thickness 1.70 mm
V-0
@Thickness 0.0669 in
UL94
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
UL94
 5VA
@Thickness 0.750 mm
5VA
@Thickness 0.0295 in
IEC 60695-11-20
Oxygen Index 53 %53 %ASTM D 2863
 
Descriptive Properties
Contains Flame RetardantYes
Heat StabilizedYes
Polymer FamilyPolyimide
Polymer TypePI
Region AvailableAmericas
 Asia/Pacific
 Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Machined
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Direct formed
DuPont Mobility and Materials Vespel® SP-22 DF Polyimide
Mitsubishi Chemical Advanced Materials Semitron™ MDS 100 PEEK
DuPont Mobility and Materials Vespel® SP-21 Polyimide, 15% Graphite Filled, Direct formed

PDTA7752 / 89864

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.