MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Luran® S KR 2863 C UV Colored ASA+PC
Categories: Polymer; Thermoplastic; ASA Polymer; Polycarbonate (PC); Polycarbonate/ASA Alloy, Unreinforced

Material Notes: Luran® S KR2863C is a blend of ASA and PC providing high impact strength and the highest heat resistance within the product line. highest heat resistance, high impact strength. Applications: Unpainted interior roof compartments, Unpainted interior mirrors.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.16 %
@Temperature 23.0 °C
0.16 %
@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation 0.60 %
@Temperature 23.0 °C
0.60 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cm0.0050 - 0.0090 in/inISO 294-4
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/in
Melt Flow  7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Volumetric; cm3/10 min; ISO 1133
 18 g/10 min
@Load 5.00 kg,
Temperature 260 °C
18 g/10 min
@Load 11.0 lb,
Temperature 500 °F
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 110 MPa16000 psiISO 2039-1
Tensile Strength, Yield 62.0 MPa8990 psiISO 527
Elongation at Break >= 50 %>= 50 %ISO 527
Elongation at Yield 4.9 %4.9 %ISO 527
Tensile Modulus 2.50 GPa363 ksiISO 527
Flexural Strength 93.0 MPa13500 psiISO 178
Poissons Ratio 0.360.36Calculated
Izod Impact, Notched 7.00 J/cm13.1 ft-lb/inASTM D256
Izod Impact, Notched (ISO)  10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact, Notched  1.70 J/cm²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0060
@Frequency 100 Hz
0.0060
@Frequency 100 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 - 90.0 µm/m-°C38.9 - 50.0 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °Fannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 109 °C228 °Fannealed 4 hours at 80°C; ISO 75
Vicat Softening Point  130 °C
@Load 5.10 kg
266 °F
@Load 11.2 lb
VST/B/50. 50C/h; ISO 306
 140 °C
@Load 1.02 kg
284 °F
@Load 2.25 lb
VST/A/50. 50C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 300 °C500 - 572 °FISO 294
Mold Temperature 80.0 °C176 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
Drying Temperature 100 - 110 °C
@Time 7200 - 14400 sec
212 - 230 °F
@Time 2.00 - 4.00 hour
 
Descriptive Properties
ColorBlack 36734
 Gray 36781
 Natural
Commercial StatusEurope
Primary Processing TechniqueInjection Molding and Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® S 777K ASA
INEOS Styrolution Luran® S 778 UV Colored ASA
INEOS Styrolution Luran® S KR 2863C Colored ASA+PC
Cossa Polimeri ESTABLEND PSA 8500 V0 Flame Retardant PC / ASA Blend
INEOS Styrolution Luran® S KR 2864 C UV Colored ASA+PC

PBASG0591 / 132224

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.