MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco 17 MG 2000 Diesel Engine Oil
Categories: Fluid; Lubricant

Material Notes: Texaco Diesel Engine Oils deliver value through:
  • Ability to maximize oil and filter life
  • Improved wear control
  • Extended drains
    • Extends oil drains in new low oil consumption GE locomotives, reducing oil costs
    • Better oxidation and viscosity control
    • Better alkalinity retention
  • Potential fuel savings. The 17 MG 2000 grade reduces fuel and oil consumption compared to single grade oils.
  • Proven superior field performance.

Texaco Diesel Engine Oils are outstanding high dispersancy, high alkalinity, 17 base number engine oils for use in diesel engines used in railroad, power generation, oil well drilling, and marine and industrial service requiring a zinc-free oil and Generation 4 LL or Generation 5 lubricant characteristics.

Texaco Diesel Engine Oils are manufactured using premium quality base oils and a nonchlorinated additive package that offers low engine wear and minimizes used oil disposal issues. Texaco Diesel Engine Oil 17 MG 2000 includes a nondispersant viscosity index improver.

New engine designs, aimed at reducing operating expenses, operate at higher combustion pressures and higher temperatures which require improved oxidation and viscosity control. In addition, new piston and ring designs call for increased alkalinity reserve to control corrosive wear and deposit formation.

Texaco Diesel Engine Oils successfully handle these new requirements by providing outstanding resistance to viscosity increase due to superior oxidation and thermal stability, and by providing a high alkalinity level (17 mg KOH/g by ASTM D 2896).

Texaco Diesel Engine Oils are recommended:

  • for use in all railroad-type diesel engines for locomotive, marine equipment, stationary electric generating plants, offshore drilling equipment, and many other applications.
  • where large medium-speed EMD or GE diesel engines are used for primary power.

Texaco Diesel Engine Oils are:
  • completely compatible with earlier Chevron Delo® railroad oils.
  • miscible with competitive railroad type oils and additive systems consistent with engine manufacturers recommended practices.

Texaco Diesel Engine Oils provide excellent performance in older locomotive types such as Sulzer, Baldwin, and ALCO. Texaco Diesel Engine Oil 17 SG 2000 is recommended:
  • for use in Caterpillar and other diesel engines operating where sulfated ash levels above 1% are acceptable.
  • where DDC engines are used for auxiliary power. Detroit Diesel Corporation approves the use of Generation 4 and 5 zinc-free railroad engine oils in these applications.

Texaco Diesel Engine Oils meet the performance requirements of:
  • API Service Categories CD1 , CD-II1, CF, CF-2
  • Caterpillar TO-2 (17 SG 2000)

Texaco Diesel Engine Oils:
  • are qualified by Electro Motive Division, General Motors, for use in engines operating under EMD factory warranty
  • are fully approved by General Electric as Extra Performance Lubricants.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222917; MSDS Number: 8614

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 28 °28 °
Viscosity Measurement 115115Viscosity Index
Kinematic Viscosity at 40°C (104°F) 138 cSt138 cSt
Kinematic Viscosity at 100°C (212°F) 15.4 cSt15.4 cSt
Ash 2.0 %2.0 %Sulfated Ash
 
Chemical PropertiesMetricEnglishComments
Total Base Number 1717ASTM D2896
 
Thermal PropertiesMetricEnglishComments
Pour Point -27.0 °C-16.6 °F
Flash Point 252 °C486 °F
 
Component Elements PropertiesMetricEnglishComments
Zinc, Zn <= 0.0010 %<= 0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco 13 SG Diesel Engine Oil
ChevronTexaco 17 SG 2000 Diesel Engine Oil
ChevronTexaco DIESELMOTIVE® Direct Injector Cleaner, for Heavy Duty Diesel Engines
Unipetrol Grade B Diesel Oil
ChevronTexaco Delo® 100 Motor Oil, SAE 30

WTEXA059 / 76938

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.