MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay FM® 300-2U Film Adhesive, psf 0.03 (147 gsm)
Categories: Polymer; Adhesive; Film

Material Notes: Description: FM® 300-2 film adhesive is a 250°F (121°C) cure version of Cytec Engineered Materials’ widely used FM® 300 film adhesive. It delivers the same superior high temperature performance, toughness and stress/strain properties of FM 300 film adhesive without requiring a 350°F (177°C) cure cycle. In addition, FM 300-2 film adhesive’s processing window includes temperatures up to 300°F (149°C) providing a unique level of flexibility from one adhesive product. FM 300-2 adhesive was developed specifically for co-cure and secondary composite bonding applications. Through innovative curative technology, the required cure temperature is reduced allowing for secondary bonding of structure far below the composite’s glass transition point. FM 300-2 film adhesive also offers optimum flow control desirable for co-cure composite bonding. In metal bond applications, FM 300-2 film adhesive provides excellent moisture and corrosion resistance in high humidity environments with a minimal reduction in mechanical properties. To achieve consistent mechanical performance as well as maximum environmental resistance in bonding metallic details, the use of pre-cured BR® 127 corrosion inhibiting primer is recommended. FM 300-2 adhesive is available as an unsupported or supported film employing both knit and random mat carriers. A low-flow version of FM 300-2 film adhesive for composite interleaving, designated FM 300-2 interleaf adhesive, is also available.

Features & Benefits:

  • 250°F (121°C) cure version of FM 300 film adhesive
  • Offers service temperatures from 67°F to 300°F (-55°C to 149°C)
  • Excellent moisture and corrosion resistance in high humidity environments with no significant reduction in mechanical properties
  • Displays similar stress/strain properties to FM 300 film adhesive under both dry and wet conditions through 220°F (104°C)
  • Ideal for co-cure and secondary composite bonding applications. Compatible with most thermoset and thermoplastic composite systems.
Applications:
  • Co-cure and secondary composite bonding
  • Vacuum-only processing common in repair applications

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %
Outgassing - Total Mass Loss 1.35 %1.35 %TWL
Collected Volatile Condensable Material 0.080 %0.080 %
Storage Temperature -18.0 °C-0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Peel Strength  6.14 kN/m
@Temperature 24.0 °C
35.0 pli
@Temperature 75.2 °F
Floating Roller, Bonded Exposure: 30 days at 160F (71C), 100% RH
 6.14 kN/m
@Temperature 24.0 °C
35.0 pli
@Temperature 75.2 °F
Floating Roller, Pre-Bond Film Exposure:15 days at 75°F (24°C), 80% RH, Bonded Exposure: 30 days at 160°F (71°C), 100% RH
 6.31 kN/m
@Temperature 24.0 °C
36.0 pli
@Temperature 75.2 °F
Floating Roller, Pre-Bond Film Exposure
 6.31 kN/m
@Temperature 121 °C
36.0 pli
@Temperature 250 °F
Floating Roller, Pre-Bond Film Exposure
 6.49 kN/m
@Temperature 121 °C
37.0 pli
@Temperature 250 °F
Floating Roller, Pre-Bond Film Exposure:15 days at 75°F (24°C), 80% RH
 6.84 kN/m
@Temperature 121 °C
39.0 pli
@Temperature 250 °F
Floating Roller, Bonded Exposure: 30 days at 160F (71C), 100% RH
 6.84 kN/m
@Temperature 121 °C
39.0 pli
@Temperature 250 °F
Floating Roller, Pre-Bond Film Exposure:15 days at 75°F (24°C), 80% RH, Bonded Exposure: 30 days at 160°F (71°C), 100% RH
 7.01 kN/m
@Temperature 24.0 °C
40.0 pli
@Temperature 75.2 °F
Floating Roller, Pre-Bond Film Exposure:15 days at 75°F (24°C), 80% RH
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Hysol PL 795-1 Film Adhesive
Henkel Hysol EA 934NA Paste Adhesive System
Henkel Hysol EA 9309.3NA Paste Adhesive System
Solvay FM® 300U Epoxy Film Adhesive
DuPont Teijin Films Mylar® LJP Polyester Film, 400 Gauge

PCYTED117 / 180419

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.