MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type S21900 (21-6-9) Stainless Steel, cold rolled sheet, 25% cold reduction
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: Austenitic, high strength, excellent corrosion resistance, and low magnetic permeability. Applications include aircraft applications such as ducting and bellows systems, tail pipes and exhaust systems, clamps, fasteners, flanges, and hydraulic tubing.

Key Words: UNS S21900, AMS 5561, ASTM A269 (XM-10), ASTM A276 (XM-10), ASTM A314 (XM-10), ASTM A412 (XM-10), ASTM A473 (XM-10), ASTM A580 (XM-10)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.83 g/cc0.283 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 326326Converted from Rockwell C hardness.
Hardness, Knoop 352352Converted from Rockwell C hardness.
Hardness, Rockwell C 3535
Hardness, Vickers 340340Converted from Rockwell C hardness.
Tensile Strength, Ultimate 1097 MPa159100 psi
 592 MPa
@Temperature 650 °C
85900 psi
@Temperature 1200 °F
 715 MPa
@Temperature 540 °C
104000 psi
@Temperature 1000 °F
 798 MPa
@Temperature 425 °C
116000 psi
@Temperature 797 °F
 877 MPa
@Temperature 315 °C
127000 psi
@Temperature 599 °F
 931 MPa
@Temperature 205 °C
135000 psi
@Temperature 401 °F
 998 MPa
@Temperature 95.0 °C
145000 psi
@Temperature 203 °F
Tensile Strength, Yield 876 MPa
@Strain 0.2 %
127000 psi
@Strain 0.2 %
 500 MPa
@Strain 0.2 %,
Temperature 650 °C
72500 psi
@Strain 0.2 %,
Temperature 1200 °F
 601 MPa
@Strain 0.2 %,
Temperature 540 °C
87200 psi
@Strain 0.2 %,
Temperature 1000 °F
 667 MPa
@Strain 0.2 %,
Temperature 425 °C
96700 psi
@Strain 0.2 %,
Temperature 797 °F
 759 MPa
@Strain 0.2 %,
Temperature 315 °C
110000 psi
@Strain 0.2 %,
Temperature 599 °F
 836 MPa
@Strain 0.2 %,
Temperature 205 °C
121000 psi
@Strain 0.2 %,
Temperature 401 °F
 881 MPa
@Strain 0.2 %,
Temperature 95.0 °C
128000 psi
@Strain 0.2 %,
Temperature 203 °F
Elongation at Break 14.5 %14.5 %in 50 mm
 5.5 %
@Temperature 205 °C
5.5 %
@Temperature 401 °F
in 50 mm
 6.0 %
@Temperature 315 °C
6.0 %
@Temperature 599 °F
in 50 mm
 8.0 %
@Temperature 650 °C
8.0 %
@Temperature 1200 °F
in 50 mm
 9.0 %
@Temperature 540 °C
9.0 %
@Temperature 1000 °F
in 50 mm
 10.5 %
@Temperature 425 °C
10.5 %
@Temperature 797 °F
in 50 mm
 12 %
@Temperature 95.0 °C
12 %
@Temperature 203 °F
in 50 mm
Modulus of Elasticity 200 GPa29000 ksiTypical for stainless steel
Machinability 30 %30 %Based on 100% machinability for AISI 1212 steel.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000730 ohm-cm0.0000730 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.7 µm/m-°C
@Temperature 25.0 - 95.0 °C
9.28 µin/in-°F
@Temperature 77.0 - 203 °F
 17.3 µm/m-°C
@Temperature 25.0 - 205 °C
9.61 µin/in-°F
@Temperature 77.0 - 401 °F
Annealed
 18.2 µm/m-°C
@Temperature 25.0 - 315 °C
10.1 µin/in-°F
@Temperature 77.0 - 599 °F
Annealed
 19.1 µm/m-°C
@Temperature 25.0 - 540 °C
10.6 µin/in-°F
@Temperature 77.0 - 1000 °F
 20.0 µm/m-°C
@Temperature 25.0 - 760 °C
11.1 µin/in-°F
@Temperature 77.0 - 1400 °F
Annealed
 20.0 µm/m-°C
@Temperature 25.0 - 870 °C
11.1 µin/in-°F
@Temperature 77.0 - 1600 °F
Annealed
 20.5 µm/m-°C
@Temperature 25.0 - 980 °C
11.4 µin/in-°F
@Temperature 77.0 - 1800 °F
Annealed
Specific Heat Capacity 0.480 J/g-°C0.115 BTU/lb-°FTypical value for stainless steel.
Thermal Conductivity  7.80 W/m-K
@Temperature -180 °C
54.1 BTU-in/hr-ft²-°F
@Temperature -292 °F
 10.9 W/m-K
@Temperature -73.0 °C
75.6 BTU-in/hr-ft²-°F
@Temperature -99.4 °F
 13.8 W/m-K
@Temperature 95.0 °C
95.8 BTU-in/hr-ft²-°F
@Temperature 203 °F
 16.1 W/m-K
@Temperature 205 °C
112 BTU-in/hr-ft²-°F
@Temperature 401 °F
 18.2 W/m-K
@Temperature 315 °C
126 BTU-in/hr-ft²-°F
@Temperature 599 °F
 20.2 W/m-K
@Temperature 425 °C
140 BTU-in/hr-ft²-°F
@Temperature 797 °F
 22.5 W/m-K
@Temperature 540 °C
156 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 24.7 W/m-K
@Temperature 650 °C
171 BTU-in/hr-ft²-°F
@Temperature 1200 °F
 26.8 W/m-K
@Temperature 760 °C
186 BTU-in/hr-ft²-°F
@Temperature 1400 °F
 28.9 W/m-K
@Temperature 870 °C
201 BTU-in/hr-ft²-°F
@Temperature 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 20 %20 %
Iron, Fe 64 %64 %
Manganese, Mn 9.0 %9.0 %
Nickel, Ni 6.0 %6.0 %
Nitrogen, N 0.23 %0.23 %
Phosphorus, P <= 0.060 %<= 0.060 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type 651 (19-9) Stainless Steel cold rolled and stress relieved, 35 HRC hardness
AISI 1018 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI Type S21904 (Alloy 21-6-9) Stainless Steel, cold rolled sheet, 25% cold reduction
ASTM A606 HSLA Steel, Cold Rolled Sheet
AISI 1022 Steel, cold rolled, 25 mm (1 in.) round

MQM22CE / 13688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.