MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayhydrol® A 2646 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Anionic polyacrylate dispersion. Waterborne, low VOC two-component polyurethane coatings in combination with aliphatic polyisocyanates.

Properties / Applications; On account of its outstanding mechanical and chemical resistance, the product is particularly suitable for the formulation of hard, high-gloss sealers for mineral substrates and reactive resins (EP, PUR). Furthermore, excellent accentuation of the grain of the substrate (e.g. colored coatings) is achieved. The binder can also be used for the formulation of high-grade low VOC coatings for use on substrates such as wood, metal, plastic, etc. The product can also be combined with other water-reducible binders. On account of the many potential co-reactants, compatibility testing should always be carried out. The high reactivity enables short drying times, which contribute to enhanced productivity. The viscosity of the product is largely governed by the pH. As the pH may decrease during storage, a decrease in viscosity is also to be expected. The viscosity can be restored to its original value by the addition of small amounts of triethanol amine. Dowanol® PnB and triethanolamine are OH-functional cosolvents/amines that react with isocyanates. They are therefore reactive thinners and not VOC-relevant pursuant to the Decopaint Directive 2004-42-EC.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccDIN EN ISO 2811-2
Volatiles 49 - 52 %49 - 52 %1g/1h/125 °C/convection oven; DIN EN ISO 3251
pH 7.0 - 8.07.0 - 8.01:4 in demineralized water; DIN ISO 976
Viscosity 1000 - 3500 cP1000 - 3500 cPD= approx. 40 s-1; DIN EN ISO 3219/A.3
 
Descriptive Properties
Content3.8%Hydroxyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayhydrol® A 2542 Polyurethane Coating

PCOVEST0157 / 201940

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.