MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayblend® FR 110 Polycarbonate/ABS Blend  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.

Applications: Housings for business machines.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: PC + ABS; Poly(Acrylonitrile-Butadiene-Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³
Moisture Absorption at Equilibrium 0.20 %0.20 %50% RH
Water Absorption at Saturation 0.70 %0.70 %
 0.70 %0.70 %
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 240 °C
20 g/10 min
@Load 11.0 lb,
Temperature 464 °F
Spiral Flow 58.0 cm
@Thickness 2.50 mm
22.8 in
@Thickness 0.0984 in
at 254°C melt temp.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ASTM D785
Tensile Strength, Ultimate 56.0 MPa8120 psiASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi
Elongation at Break 90 %90 %ASTM D638
Elongation at Yield 4.0 %4.0 %
Tensile Modulus 2.60 GPa377 ksi
Flexural Yield Strength 95.0 MPa13800 psiat 5% strain; ASTM D790
Flexural Modulus 2.70 GPa392 ksiASTM D790
Izod Impact, Notched 7.50 J/cm
@Thickness 3.20 mm
14.1 ft-lb/in
@Thickness 0.126 in
ASTM D256
Impact Test 52.0 J
@Thickness 3.20 mm
38.4 ft-lb
@Thickness 0.126 in
Instrumented Total Impact; 3.2 mm thick, 12.5 mm dart, 75 mm clamp, 6.7 m/s; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm762 kV/in
Dissipation Factor  0.0030
@Frequency 100 Hz
0.0030
@Frequency 100 Hz
 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
60 - 120 sec
@Thickness 0.118 in
UL Rating PLC 6 (60-120 sec)
Comparative Tracking Index 300 V300 V
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness 3.00 mm
60 - 120 sec
@Thickness 0.118 in
UL Rating PLC 1 (60-120 sec)
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 2.00 mm
>= 120 arcs
@Thickness 0.0787 in
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
@Thickness 3.00 mm
>= 5.91 in/min
@Thickness 0.118 in
UL Rating PLC 4 (>150 mm/min.)
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 76.0 µm/m-°C
@Temperature 20.0 °C
42.2 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °F
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °F
Vicat Softening Point 108 °C226 °F
UL RTI, Electrical 95.0 °C203 °F
UL RTI, Mechanical with Impact 85.0 °C185 °F
UL RTI, Mechanical without Impact 85.0 °C185 °F
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Oxygen Index 30 %30 %
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 270 °C428 - 518 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade
Covestro Bayblend® FR3010 HF PC/ABS Blend
Covestro Bayblend® FR3010 IF PC/ABS Blend
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy
Covestro Bayblend® FR 2000 Polycarbonate/ABS Blend

PBA025 / 26652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.